Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Linear Low Density Polyethylene (LLDPE), Compounding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Compounding Resin
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Linear Low Density Polyethylene (LLDPE), Compounding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Compounding Resin". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.890 - 0.926 g/cc
0.0322 - 0.0335 lb/in³
Average value: 0.921 g/cc Grade Count:22
Particle Size 400 - 1200 µm
400 - 1200 µm
Average value: 771 µm Grade Count:7
Environmental Stress Crack Resistance 1.00 - 1000 hour
1.00 - 1000 hour
Average value: 177 hour Grade Count:6
Melt Flow 1.40 - 70.0 g/10 min
1.40 - 70.0 g/10 min
Average value: 24.2 g/10 min Grade Count:27
Mechanical Properties Metric English Comments
Hardness, Shore D 41.0 - 51.0
41.0 - 51.0
Average value: 46.4 Grade Count:14
Tensile Strength, Ultimate 7.45 - 21.0 MPa
1080 - 3050 psi
Average value: 13.1 MPa Grade Count:7
Tensile Strength, Yield 10.0 - 23.0 MPa
1450 - 3340 psi
Average value: 13.3 MPa Grade Count:9
Elongation at Break 40.0 - 800 %
40.0 - 800 %
Average value: 326 % Grade Count:10
Flexural Modulus 0.200 - 0.480 GPa
29.0 - 69.6 ksi
Average value: 0.287 GPa Grade Count:5
Secant Modulus 0.230 - 0.448 GPa
33.4 - 65.0 ksi
Average value: 0.354 GPa Grade Count:5
Izod Impact, Notched 4.43 - 5.00 J/cm
8.30 - 9.37 ft-lb/in
Average value: 4.81 J/cm Grade Count:3
Dart Drop, Total Energy 29.0 - 37.0 J

@Temperature -40.0 - -40.0 °C
21.4 - 27.3 ft-lb

@Temperature -40.0 - -40.0 °F
Average value: 33.0 J Grade Count:2
Thermal Properties Metric English Comments
Melting Point 112 - 124 °C
234 - 255 °F
Average value: 121 °C Grade Count:16
Vicat Softening Point 88.0 - 94.0 °C
190 - 201 °F
Average value: 91.8 °C Grade Count:10
Brittleness Temperature -80.0 - -68.0 °C
-112 - -90.4 °F
Average value: -74.3 °C Grade Count:7
Processing Properties Metric English Comments
Melt Temperature 160 - 230 °C
320 - 446 °F
Average value: 199 °C Grade Count:3