Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | >= 245 °C | >= 473 °F | Unannealed; ASTM D648 |
PolyOne Stat-Tech™ X ST6600-0040 ES FR Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | >= 245 °C @Thickness 3.18 mm |
>= 473 °F @Thickness 0.125 in |
Annealed; ASTM D648 |
PolyOne Trilliant™ HC HC9820-0030 RS Natural Polyetheretherketone (PEEK) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ISO 75 |
Nilit FRIANYL A63 FK 1020 Nylon 6.6 for injection molding, 10% glass fiber and 20% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ISO 75 |
Nilit FRIANYL A63 FK 2010 Nylon 6.6 for injection molding, 20% glass fiber and 10% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ISO 75 |
Nilit FRIANYL A63 HH-FK 1020 Nylon 6.6 for injection molding, 10% glass fiber and 20% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Nilit Polynil® P50L Externally Lubricated Nylon 66 Description: Polynil P50L is a general purpose injection molding grade that is widely used for gears, bearings, fasteners, clips. It is also suited for monofilament extrusion.Key characteristics: Ex.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | |
Radici Radilon® A CF350 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | DIN 53461; ASTM D648 |
Kolon KOPA® KN333G15 G/F Reinforced Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Kolon KOPA® KN333G15SIBL G/F Reinforced Nylon 66 High strength, high toughnessApplications Relay coversInformation provided by API-Kolon. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Kolon KOPA® KN333HB40HFBL Hybrid Nylon 66 High flow, dimensionally stableApplications Fans & ShroudsInformation provided by API-Kolon. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ISO 75-1, -2 |
Lanxess Durethan® DP 2-2240/15 H2.0 901510 Nylon 66, 15% Glass Fiber PA 66, 15% glass fibers, blow molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRILOY RF203 PA 66 (Europe-Africa-Middle East) LNP* LUBRILOY* RF203 is a compound based on PA 66 resin containing Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C @Thickness 3.20 mm |
473 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics LNP Thermocomp RX06423 PA 66 LNP* Thermocomp* RX06423 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized.This data was supplied b.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Plastics Group Polifil® 71MR Mineral-Reinforced Nylon 6/6 (DAM) Polifil® GFN/MRN 6/6 reinforced series of compounds offer superior strength, rigidity and creep resistance. Glass fibers provide excellent thermal and dimensional stability while maintaining good h.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | Absolute Drying; ASTM-D648 |
Toyobo GLAMIDE® TY-835TC Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Toyobo Vylopet® EMC120S Glass Reinforced Polyester, Standard Grade Key Feature: Flame retardant V-0 UL-94 classApplications: Electric and electronic componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strengt.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Toyobo VYLOPET® EMC132-01 Injection Molding Polyester Resin, Flame Resistant Applications: Relay partsFeatures: Excellent arc resistanceFlame resistanceInformation provided by Toyobo. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ISO 75 |
Ter Hell Plastic Terez® PA 6.6 HT 7110 GF 41 FL-HF/2 Polyamide 66 Copolymer, 41% Glass Fiber Description: Partly aromatic Polyamide 6.6 Copolymer, 41% glass fiber reinforced and flame retardants.Application:Stiff molding parts with high stiffness by outstanding thermal stability, reduced w.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ISO 75-1/-2 |
DuPont Performance Polymers Rynite® 515CS BK575M PET Rynite® 515CS BK575M is a 15% glass fiber reinforced, black polyethylene terephthalate resin modified for improved color stability after heat aging.Information provided by DuPont Performance Polyme.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | Edgew 120x10x4, sp=100 mm; ISO 75/Be |
Eurostar Starflam AF430B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR430B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ISO 75 |
Eurotec® Tecomid® NA43 GR25 NL TD43 PA6.6, 25% glass fiber reinforced, flame retardant - red phosphorus free, high impact, heat stabilized, natural Information provided by Eurotec® |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
E-Polymers Tekaster® F615GFR , Flame Retardant, 30% Glass Reinforced PET 30% Glass Fiber Reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ISO 75-1/-2 |
DSM Akulon® S223-HM8 Nylon 66-40% Mineral Reinforced (European and Asian Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ISO R75 |
Arkema Group Orgalloy® RS 6635 A Polyamide 6.6 Alloy 35% Glass Fiber reinforced Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | HDT/B; ISO 75-1/2 |
Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Dry, 60% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Cheng Yu Plastic E2330 Flame Retardant PET, 30% Glass Fiber |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Adell AW-37 Nylon 66, 35% Glass Reinforced; Superior Finish Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | ASTM D648 |
Celanese Impet® 740 PET, 45% Glass/Mineral Reinforced Information provided by Celanese Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | Unannealed; ISO 75-2/B |
Ascend Performance Materials Vydyne® 75HF Nylon 66/6, Heat Stabilized, DAM Vydyne® 75HF is a medium-high-viscosity, heat-stabilized PA66/6 copolymer resin designed for extrusion applications. It is available in natural color only. Vydyne 75HF resin offers a well-balanced .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 245 °C | 473 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East) Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |