Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 473 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) >= 245 °C
>= 473 °F
Unannealed; ASTM D648
PolyOne Stat-Tech™ CTX-20SS 107/000 Keytec Blue Polyamide 6/12 Copolymer (Nylon 6/12)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Deflection Temperature at 0.46 MPa (66 psi) >= 245 °C
>= 473 °F
Unannealed; ASTM D648
PolyOne Stat-Tech™ X ST6600-0040 ES FR Black Polyamide 66 (Nylon 66)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Deflection Temperature at 0.46 MPa (66 psi) >= 245 °C
>= 473 °F
Unannealed; ASTM D648
PolyOne Stat-Tech™ X ST6600-0041 ES NHFR Black Polyamide 66 (Nylon 66)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Deflection Temperature at 0.46 MPa (66 psi) >= 245 °C

@Thickness 3.18 mm
>= 473 °F

@Thickness 0.125 in
Annealed; ASTM D648
PolyOne Trilliant™ HC HC9820-0030 RS Natural Polyetheretherketone (PEEK)
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead..
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ISO 75
Nilit FRIANYL A63 FK 2010 Nylon 6.6 for injection molding, 20% glass fiber and 10% glass ball reinforced
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
Radici Radilon® A RV150 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
Unannealed; ISO 75-2
PolyOne Bergamid™ PA66 C20 Black Polyamide 66 (Nylon 66)
Product code EM00000364BIInformation provided by PolyOne
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
Unannealed; ASTM D648
PolyOne Edgetek® X PS-154200101 WHITE Polybutylene Terephthalate (PBT)
Information provided by PolyOne
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ASTM D648
Samyang Tripet® 2550GN45 Polyethylene Terephthalate, 45% Glass Fiber Reinforced, Flame Retardant  (discontinue
TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll information..
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ASTM D648
Nilit Polynil® P50L Externally Lubricated Nylon 66
Description: Polynil P50L is a general purpose injection molding grade that is widely used for gears, bearings, fasteners, clips. It is also suited for monofilament extrusion.Key characteristics: Ex..
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ISO 75
Nilit FRIANYL A63 HH-FK 2020 Nylon 6.6 for injection molding, 20% glass fiber and 20% glass ball reinforced
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
Radici Radilon® A CF350 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ASTM D648
Kolon KOPA® KN333HB40HFBL Hybrid Nylon 66
High flow, dimensionally stableApplications Fans & ShroudsInformation provided by API-Kolon.
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ISO 75-1,-2
Lanxess Durethan® AKV 15 FN 00 000000 Nylon 66, 12% Glass Fiber
PA 66, 12% glass fiber, injection molding, halogen free flame retardantInformation provided by LANXESS.
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ISO 75-1, -2
Lanxess Durethan® DP 2-2240/15 H2.0 901510 Nylon 66, 15% Glass Fiber
PA 66, 15% glass fibers, blow molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS.
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP LUBRILOY RF203 PA 66 (Europe-Africa-Middle East)
LNP* LUBRILOY* RF203 is a compound based on PA 66 resin containing Glass Fiber, Proprietary Lubricant. Added features include: Internally Lubricated.
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
SABIC Innovative Plastics LNP THERMOCOMP RB00A PA 66 (Europe-Africa-Middle East)
50% glass beads filled Polyamide 66 injection moulding resin.
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ISO 75
Polyram RamLloy A300NT Nylon 66/Polypropylene Alloy, 30% Glass Fiber Reinforced
Nylon 66/PP alloy 30% glass fiber reinforced for injection molding applications.Information provided by Polyram.
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ISO 75
Polyram RamSter PE321G6 PET, 30% Glass Fiber, Flame Retardant
30% Glass fiber reinforced, flame retardant V-0 PET for injection molding applications.Information provided by Polyram.
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
0.455 MPa
Toyobo ECOVYLOPET® EMC2330 PET Bottle Recycling Grade, 30% Glass Reinforced
Features: PET Bottle Recycling Grade, 30% Glass Fiber Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo..
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ASTM D648
Toyobo VYLOPET® EMC132-01 Injection Molding Polyester Resin, Flame Resistant
Applications: Relay partsFeatures: Excellent arc resistanceFlame resistanceInformation provided by Toyobo.
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ASTM D648
Toyobo VYLOPET® EMC355 Injection Molding Polyester Resin, Glass Reinforced
Applications: HousingsBracketsGear casesFeatures: High RigidityGlass fiber reinforcementInformation provided by Toyobo.
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ASTM D648
Cheng Yu Plastic N66C3 Nylon 66, 30% Mineral Reinforced
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ASTM D648
Cheng Yu Plastic NG1150S Nylon 66, 15% Glass Fiber Reinforced
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ISO 75-1/-2
DSM Akulon® S223-HM8 (Dry) 40% Mineral Reinforced, Heat Stabilized Nylon 66 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ISO 75-1/-2
DSM Arnite® AV2 340 PET-20% Glass Reinforced (European Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ISO 75-1/-2
DSM Akulon® S223-HM8 Nylon 66-40% Mineral Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ISO R75
Arkema Group Orgalloy® RS 6630 Polyamide 6.6 Alloy 30% Glass Fiber reinforced
Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
Arkema Group Orgalloy® RS 6635 A Nylon 66 Alloy, 35% Glass Fiber (Conditioned)
RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie..
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
HDT/B; ISO 75-1/2
Akro-Plastic Akroloy® PA GF 40 (2845) PA 6.6 & PA6I/6T Dry, 40% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..