Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ISO 75 |
Eastman Eastar GN125 Copolyester, Natural
(discontinued **) Eastar Copolyester GN125 is a glycol modified polyethylene terephthalate (PET) that contains an ultraviolet light inhibitor. This product is recommended for indoor applications requiring enhanced co.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ASTM D648 |
Eastman Eastar GN125 Copolyester, Natural
(discontinued **) Eastar Copolyester GN125 is a glycol modified polyethylene terephthalate (PET) that contains an ultraviolet light inhibitor. This product is recommended for indoor applications requiring enhanced co.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ISO 75 |
Eastman 9921 PET Injection Molded
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ASTM D648 |
Eastman 9921P PET Injection Molded
(discontinued **) Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 - 147 °C | 156 - 297 °F | Average value: 111 °C Grade Count:5 |
Overview of materials for Nylon 11, Flexible Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Flexible Tubing Grade". Each property range of values reported is minimum and maximum values o.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | |
LyondellBasell Lupolen® 3652 D SW 00413 MDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | |
LyondellBasell Lupolen® 4152 D SW 00413 HDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ISO 75 |
Manifattura Cattaneo PVC HI Polyvinyl Chloride Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ISO 75 |
GEHR Plastics PE-ELS® Polyethylene HDPE A variant of PE-HD with improved electrical conductivity.Polyethylene has a good chemical resistance against almost all acids and bases, detergents and hot water. PE has good insulation properties a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ISO 75 |
GEHR Plastics PE-HD Polyethylene HDPE Polyethylene has a good chemical resistance against almost all acids and bases, detergents and hot water. PE has good insulation properties and is easy to weld. The operating temperature is from -50.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ASTM D648 |
Ineos K46-06-185 HDPE K46-06-185 is a natural high molecular weight, high-density copolymer polyethylene developed for automotive fuel tanks. It combines excellent processability and outstanding physical performance, par.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ISO 75 |
LyondellBasell Hifaxâ„¢ CA187 Thermoplastic Olefin Resin Key Features: medium melt flow, medium modulus, paintable thermoplastic elastomeric olefin resin, excellent paintability, excellent surface appearance, good impact and stiffness balanceApplications:.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Stat-kon TD000 LNP* Stat-kon* TD000 is a compound based on Polyurethane resin. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ASTM D648 |
Lubrizol Estaloc® 61225 Polyester-Type Thermoplastic Alloy Type: Estaloc® 61225 Alloy RETPU is a polyester-type thermoplastic alloy.Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact.Uses: Injection molding.Availa.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ASTM D648 |
Eastman Aspira EN177 Copolyester Resin for Extrusion Blow Molding Applications:Beverage packagingConsumer packagingFood packagingPersonal care packagingKey Attributes:BPA-freeCompatible with high-output manufacturing platformsExcellent clarityHigh gloss appearance.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ASTM D648 |
Eastman Eastar EN001 Copolyester Eastar EN001 Copolyester is a thermoplastic polyester copolymer. Eastar EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming pro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ASTM D648 |
Eastman Eastar EN010 Copolyester Eastar copolyester EN010 is used primarily in molded thick wall European applications.Applications/UsesPackagingInjection moldingContainers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ASTM D648 |
Eastman Eastar EN076 Copolyester Eastar Copolyester EN076 is recommended for the thick-walled containers that are prevalent in the cosmetics and personal care markets. This copolyester offers good processability with the benefits o.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | |
Eastman Eastar GN007 PETG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ASTM D648 |
Eastman Eastar MN021 Copolyester Eastar copolyester MN021 is a thermoplastic condensation copolymer produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. It has been crystalliz.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ASTM D648 |
Eastman Eastar MN058 Copolyester Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN058 Copolyester is a medical gra.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ASTM D648 |
Eastman Eastar MN059 Copolyester Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN059 Copolyester is a medical gra.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ASTM D648 |
Eastman Eastar MN200 Copolyester Eastar Copolyester MN200 is an amorphous copolyester with excellent flow characteristics as well as radiation resistance and chemical resistance.Applications/UsesMedical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ASTM D648 |
Eastman Tenite Acetate 105E1R26029 Clear, Trsp Cellulose Acetate TENITE cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of TENITE cellulosi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ISO 75 |
Eastman Eastar GN071 Natural PETG Copolyester EASTAR GN071 Copolyester is used for injection molding applications. It is sparkling clear, tough, chemical resistant, odor free, versatile, easy to work with and affordable. Cleaning solutions wi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ASTM-D648 |
Braskem GD5150K HDPE High Density Extrusion Polyethylene GD5150K is a high-density polyethylene specially developed for the manufacturing of insulation for wires and cables demanding high extrusion velocity. It has medium molar mass, shows good dielectric.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | |
Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11/xx,E,18-002Transparent and flexible copolymer for tubes extrusion. Additive free.High flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 - 91.0 °C | 156 - 196 °F | Average value: 82.2 °C Grade Count:13 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ASTM D648 |
Eastman 9921W PET Injection Molded
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 69.0 °C | 156 °F | ASTM D648 |
LyondellBasell Hifax™ ETA-3131 Thermoplastic Olefin Resin Key Features: medium melt flow, medium modulus thermoplastic olefin resin, excellent impact and stiffness balance, excellent processabilityApplications: automotive filler and valance panels, lower a.. |