Thermal Properties Metric English Comments
UL RTI, Mechanical with Impact 140 °C

@Thickness 0.860 mm
284 °F

@Thickness 0.0339 in
UL 746B
DuPont Performance Polymers Rynite® FR515 BK507 PET  (Unverified Data**)
Rynite® FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm(0.03in). Has a 140C temp index. Excellent balance of electr..
UL RTI, Mechanical with Impact 140 °C
284 °F
UL 746B
Glastic Laminates/Shapes 1580 Polyester Laminate
Data provided by Glastic Corporation.NEMA GPO-3. Developed to meet the television industry's safety assurance requirements.
UL RTI, Mechanical with Impact 140 °C
284 °F
UL 746B
SABIC Innovative Plastics Valox® 420 PBT (Asia Pacific)
30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors.
UL RTI, Mechanical with Impact 140 °C
284 °F
UL 746B
SABIC Innovative Plastics Valox® 420R PBT (Asia Pacific)
30% GR, ex strength/stiffness/dimensional stability; heat resistance. Appliance handles, spotlights, electric motors, etc. Internal mold release.This data was supplied by SABIC-IP for the Asia Pacif..
UL RTI, Mechanical with Impact 140 °C
284 °F
UL 746B
SABIC Innovative Plastics Valox® 735 PBT
40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only.This data was supplied by SABIC-IP for the Americas re..
UL RTI, Mechanical with Impact 140 °C
284 °F
UL 746B
SABIC Innovative Plastics Valox® 735 PBT (Asia Pacific)
40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only.
UL RTI, Mechanical with Impact 140 °C
284 °F
UL 746B
SABIC Innovative Plastics Valox® 735 PBT+PET
40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only.
UL RTI, Mechanical with Impact 140 °C
284 °F
UL 746B
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
UL RTI, Mechanical with Impact 140 °C
284 °F
UL 746B
SABIC Innovative Plastics Valox® ENH4565 PBT (Europe-Africa-Middle East)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
UL RTI, Mechanical with Impact 140 °C
284 °F
UL 746B
SABIC Innovative Plastics Valox® HR426 PBT
AUTOMOTIVE. 30% GR, hydrolytically stable PBT. Excellent strength, stiffness and dimensional stability.
UL RTI, Mechanical with Impact 140 °C
284 °F
UL 746B
SABIC Innovative Plastics Valox® HR426 PBT (Asia Pacific)
AUTOMOTIVE. 30% GR, hydrolytically stable PBT. Excellent strength, stiffness and dimensional stability.
UL RTI, Mechanical with Impact 140 °C
284 °F
UL 746B
SABIC Innovative Plastics Valox® IQ420 PBT
Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc.
UL RTI, Mechanical with Impact 140 °C
284 °F
UL 746B
SABIC Innovative Plastics Valox® IQ420 PBT (Asia Pacific)
Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc.
UL RTI, Mechanical with Impact 140 °C
284 °F
UL 746B
SABIC Innovative Plastics Valox® IQ420 PBT (Europe-Africa-Middle East)
Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc.
UL RTI, Mechanical with Impact 140 °C
284 °F
UL 746B
SABIC Innovative Plastics Valox® EXVX1403 PBT (Asia Pacific)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
UL RTI, Mechanical with Impact 140 °C
284 °F
UL 746B
SABIC Innovative Plastics Valox® IQNH4550 PBT (Europe-Africa-Middle East)
Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT..
UL RTI, Mechanical with Impact 140 °C
284 °F
UL 746B
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific)
Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT..
UL RTI, Mechanical with Impact 140 °C

@Thickness 0.750 mm
284 °F

@Thickness 0.0295 in
UL 746B
DuPont Performance Polymers Rynite® 408 BK515 PET
Rynite® 408 BK515 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness and temperature resistance.Info..
UL RTI, Mechanical with Impact 140 °C
284 °F
UL 746B
DuPont Performance Polymers Rynite® 530 BK503 PET  (Unverified Data**)
Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, ..
UL RTI, Mechanical with Impact 140 °C

@Thickness 0.810 mm
284 °F

@Thickness 0.0319 in
UL 746B
DuPont Performance Polymers Rynite® 530 BK503 PET  (Unverified Data**)
Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, ..
UL RTI, Mechanical with Impact 140 °C

@Thickness 1.50 mm
284 °F

@Thickness 0.0591 in
UL 746B
DuPont Performance Polymers Rynite® 530 BK503 PET  (Unverified Data**)
Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, ..
UL RTI, Mechanical with Impact 140 °C

@Thickness 2.00 mm
284 °F

@Thickness 0.0787 in
UL 746B
DuPont Performance Polymers Rynite® 530 BK503 PET  (Unverified Data**)
Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, ..
UL RTI, Mechanical with Impact 140 °C

@Thickness 6.00 mm
284 °F

@Thickness 0.236 in
UL 746B
DuPont Performance Polymers Rynite® 530 BK503 PET  (Unverified Data**)
Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, ..