Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 140 °C @Thickness 0.860 mm |
284 °F @Thickness 0.0339 in |
UL 746B |
DuPont Performance Polymers Rynite® FR515 BK507 PET
(Unverified Data**) Rynite® FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm(0.03in). Has a 140C temp index. Excellent balance of electr.. |
|||
UL RTI, Mechanical with Impact | 140 °C | 284 °F | UL 746B |
Glastic Laminates/Shapes 1580 Polyester Laminate Data provided by Glastic Corporation.NEMA GPO-3. Developed to meet the television industry's safety assurance requirements. |
|||
UL RTI, Mechanical with Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 420 PBT (Asia Pacific) 30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors. |
|||
UL RTI, Mechanical with Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 420R PBT (Asia Pacific) 30% GR, ex strength/stiffness/dimensional stability; heat resistance. Appliance handles, spotlights, electric motors, etc. Internal mold release.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
UL RTI, Mechanical with Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 735 PBT 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only.This data was supplied by SABIC-IP for the Americas re.. |
|||
UL RTI, Mechanical with Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 735 PBT (Asia Pacific) 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only. |
|||
UL RTI, Mechanical with Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 735 PBT+PET 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only. |
|||
UL RTI, Mechanical with Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
UL RTI, Mechanical with Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® ENH4565 PBT (Europe-Africa-Middle East) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
UL RTI, Mechanical with Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® HR426 PBT AUTOMOTIVE. 30% GR, hydrolytically stable PBT. Excellent strength, stiffness and dimensional stability. |
|||
UL RTI, Mechanical with Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® HR426 PBT (Asia Pacific) AUTOMOTIVE. 30% GR, hydrolytically stable PBT. Excellent strength, stiffness and dimensional stability. |
|||
UL RTI, Mechanical with Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® IQ420 PBT Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
UL RTI, Mechanical with Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® IQ420 PBT (Asia Pacific) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
UL RTI, Mechanical with Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® IQ420 PBT (Europe-Africa-Middle East) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
UL RTI, Mechanical with Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® EXVX1403 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
UL RTI, Mechanical with Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® IQNH4550 PBT (Europe-Africa-Middle East) Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT.. |
|||
UL RTI, Mechanical with Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific) Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT.. |
|||
UL RTI, Mechanical with Impact | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Rynite® 408 BK515 PET Rynite® 408 BK515 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness and temperature resistance.Info.. |
|||
UL RTI, Mechanical with Impact | 140 °C | 284 °F | UL 746B |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |
|||
UL RTI, Mechanical with Impact | 140 °C @Thickness 0.810 mm |
284 °F @Thickness 0.0319 in |
UL 746B |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |
|||
UL RTI, Mechanical with Impact | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |
|||
UL RTI, Mechanical with Impact | 140 °C @Thickness 2.00 mm |
284 °F @Thickness 0.0787 in |
UL 746B |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |
|||
UL RTI, Mechanical with Impact | 140 °C @Thickness 6.00 mm |
284 °F @Thickness 0.236 in |
UL 746B |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |