Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -18.0 °C | -0.400 °F | ASTM D746-98 |
Rogers Corporation Poron® 4790-92-20 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | ASTM D746 |
S&E Specialty Polymers TufTech™ GA-8705-03 Natural Gloss PVC Compound Application: 75°C lead free, RoHS compliant riser jacketing compound.Information provided by S&E Specialty Polymers |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | ASTM D746 |
S&E Specialty Polymers GA-1042LF PVC Application: UL bulletinized PVC based compound, suitable for injection molding application.Information provided by S&E Specialty Polymers |
|||
Brittleness Temperature | <= -18.0 °C | <= -0.400 °F | ASTM D746 |
S&E Specialty Polymers TufTech™ GA-93-016AGH PVC Compound Application: A RoHS Compliant, Flame Retardant 60/75?C Jacketing Compound.Information provided by S&E Specialty Polymers |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | ASTM D746 |
LyondellBasell Montell 0300 Polybutene Key Features: highly isotactic, semi-crystalline homopolymer, good creep resistance, good environmental crack resistance, miscible with polypropylenesApplications: packaging industry, minor additive.. |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | ASTM D746 |
LyondellBasell Montell 0800 Polybutene Key Features: highly isotactic, semi-crystalline homopolymer, good creep resistance, good environmental crack resistance, miscible with polypropylenes, FDA acceptableApplications: concrete carrierMe.. |
|||
Brittleness Temperature | <= -18.0 °C | <= -0.400 °F | ASTM D 746 |
Karina 813-IS-SD Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | ASTM D746 |
LyondellBasell DP 0110M Polybutene Key Features: highly isotactic, semi-crystalline nucleated homopolymer, good creep resistance, good environmental stress crack resistance, FDA acceptable, easily dispersibleApplications: packaging i.. |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | ASTM D746 |
Teknor Apex APEX® 84854 Polyvinyl Chloride, Flexible Notes: 105°C Insulation; RoHS CompliantFeatures: Flame Retardant; High Heat Resistant Uses: InsulationAgency Ratings: UL 62 Forms: Pellets Wire Types: SJT; ST; SVTInformation Provided by Teknor A.. |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | ASTM D746 |
Teknor Apex Flexalloy® 9607-96 Polyvinyl Chloride, Elastomer Notes: 105°C Jacket; RoHS Compliant Uses Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | |
Daikin DAI-EL G-575 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 70% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Low permeability to gasoline and a.. |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | |
Daikin DAI-EL G-716 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Minimal compression set and fast vulcanization.Information provided by.. |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | |
Daikin DAI-EL G-781 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PMS 78 Flexible PVC, Extrusion Gas pipes |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | ASTM D746 |
Colorite Polymers 9034 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | ASTM D746 |
Colorite Polymers 9234 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PH 75/AS Flexible PVC, Transparent Extrusion Food belt carriers |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PHS 75/B Flexible PVC, Transparent Extrusion Pipes for gasoline CAVIS |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | |
AlphaGary PVC GM 8015-M Natural LCF Polyvinyl Chloride Thermoplastic A lead / cadmium free, 105°C, UL-94 V-O rated, electrical grade molding compound |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | ASTM D-746 |
Axiall 8910 Moldings & Extrusions Flexible PVC Extrusion compound especially formulated for extruded T-moldings, tubings, and other shapes where uniform flow through the die is required.Information provided by Georgia GulfGeorgia Gulf became Axi.. |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | |
AlphaGary GW 2462 H VW1 LCF Flame Retardant Polyvinyl Chloride 105°C rated semi-rigid insulation compound |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | |
AlphaGary GW 2463 H VW1 LCF Flame Retardant Polyvinyl Chloride 105°C rated compound for thin wall ribbon cable application |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | ASTM D-746 |
Axiall 19481 Wire & Cable Flexible PVC 105°C, VW-1 rated non-lead stabilized insulation. Best suited for small gauge, 1/64 wall applications. UL approved for TW, THW, THHW, THHN-THWN insulation.Information provided by Georgia GulfGeor.. |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | ASTM D-746 |
Axiall 19940-03 Wire & Cable Flexible PVC THHN-THWN circuit sizes. Best suited for 1/64 wall, 18 AWG and smaller. UL recognized for THHN, THW, THWN, TW. Oil resistant II and VW-1 rated.Information provided by Georgia GulfGeorgia Gulf bec.. |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W1100L-xx92FRD Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable W1100L-xx92FRDA Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Brittleness Temperature | -18.0 °C | -0.400 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PM 84 Flexible PVC, Lead Free Pipes and profiles |