Material Notes:
Medium mineral filled, weather stabilityInformation provided by PolyPlastic Group.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Melt Flow 3.5 g/10 min

@Load 5.00 kg,
Temperature 190 °C
3.5 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
ISO 868
Tensile Strength at Break 6.50 MPa
943 psi
ISO 37
Elongation at Break 650 %
650 %
ISO 37
Compression Set 40 %

@Temperature 70.0 °C,
Time 79200 sec
40 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D 395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 °C
194 °F
Dynamic
135 °C
275 °F
Static
Brittleness Temperature -55.0 °C
-67.0 °F
Processing Properties Metric English Comments
Melt Temperature 190 - 200 °C
374 - 392 °F
Mold Temperature 10.0 - 50.0 °C
50.0 - 122 °F