Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 70.0 - 120 °C
158 - 248 °F
Injection; ISO 75-C
Raschig Group RALUPOL® 2200 UP Polyester
Organically filled polyester molding compound. Low post-shrinkage, good electrical values and mechanical properties, high surface quality and good color stability (non-yellowing). This product meets..
Deflection Temperature at 8.0 MPa 70.0 - 130 °C
158 - 266 °F
Injection; ISO 75-C
Raschig Group RALUPOL® 8601 UP
Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic moulding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical stren..
Deflection Temperature at 8.0 MPa 70.0 - 130 °C
158 - 266 °F
Injection; ISO 75-C
Raschig Group RALUPOL® 8602 UP
Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic molding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical streng..
Deflection Temperature at 8.0 MPa 70.0 °C
158 °F
ISO 75-1,-2
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers
PA 66, 15% glass fibers, injection molding, heat-ageing stabilized
Deflection Temperature at 8.0 MPa 70.0 °C
158 °F
ISO 75-1/-2
Lanxess Pocan® B 4215 000000 PBT, 12% Glass Fiber
PBT, 12% glass fibers, injection molding, flame retardant
Deflection Temperature at 8.0 MPa 70.0 °C
158 °F
ISO 75-1/-2
Lanxess Pocan® KU 2-7209 Z 000000 PBT, 15% Glass Fiber
PBT, 15% glass fibers, injection molding, flame retardant, impact modified
Deflection Temperature at 8.0 MPa 70.0 °C
158 °F
ISO 75-1/-2
Lanxess Durethan® AKV 15 000000 Nylon 66, 15% Glass Fiber
PA 66, injection molding grade, 15% glass fibers
Deflection Temperature at 8.0 MPa 70.0 °C
158 °F
ISO 75-1/-2
Lanxess Durethan® AKV 15 H2.0 901510 Nylon 66, 15% Glass Fiber
PA 66, injection molding grade, 15% glass fibers, good heat-ageing resistance
Deflection Temperature at 8.0 MPa 70.0 °C
158 °F
ISO 75-1/-2
Lanxess Pocan® BF 8230 000000 PBT, 30% Glass Fiber
PBT, 30% glass spheres/glass fibers, injection molding, flame retardant, low tendency to warp, improved surface finish
Deflection Temperature at 8.0 MPa 70.0 °C
158 °F
ISO 75-1/-2
EMS-Grivory Grivory® AG-30 LF 15 PA66-(GF+Z)45
Product description: Grilon AG-30 LF 15 black 9832 is a heat stabilized, normal viscosity PA66 injection molding grade with 30% glass fibers and 15% of a combination of PTFE and silicone. Grilon AG-..
Deflection Temperature at 8.0 MPa 70.0 °C
158 °F
ISO 75-1/-2
EMS-Grivory Grivory® BG-25 HM PA6-GF25
Product description: Grilon BG-25 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 25% glass fibers. Grilon BG-25 HM has the following important prop..
Deflection Temperature at 8.0 MPa 70.0 °C
158 °F
ISO 75-1/-2
EMS-Grivory Grivory® GVN-35H black 9915 PA*-GF35
Product description: Grivory GVN-35H is a 35% glass-fiber reinforced, impact-modified engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic c..
Deflection Temperature at 8.0 MPa 70.0 °C
158 °F
ISO 75-1/-2
EMS-Grivory Grivory® TSG-30/4 LF 15 PA666-(GF+Z)45
Product description: Grilon TSG-30/4 LF 15 natural is a normal viscosity, heat stabilized PA 66 + PA 6- molding type with 30% glass fibre reinforcement and 15% of a combination PTFE and siliconoil. ..
Deflection Temperature at 8.0 MPa 70.0 °C
158 °F
ISO 75-1/-2
EMS-Grivory Grivory® TSM-30 PA666-MD30
Product description: Grilon TSM-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% mineral. Grilon TSM-30 has the following important properties: Excellent surface..