Product description: Grilon AG-30 LF 15 black 9832 is a heat stabilized, normal viscosity PA66 injection molding grade with 30% glass fibers and 15% of a combination of PTFE and silicone. Grilon AG-30 LF 15 black 9832 has the following important properties: High stiffnessHigh wear resistanceExcellent sliding friction characteristics Grilon AG-30 LF 15 black 9832 is used typically for slide bearing applications such as shaft bearing rings, gears and planetary gears.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ISO 1183
Water Absorption 5.0 %
5.0 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
conditioned; ISO 527-1/-2
100 MPa
14500 psi
dry; ISO 527-1/-2
Elongation at Break 4.0 %
4.0 %
dry; ISO 527-1/-2
8.0 %
8.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 3.00 GPa
435 ksi
conditioned; ISO 527-1/-2
6.50 GPa
943 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 4.00 J/cm²
19.0 ft-lb/in²
dry; ISO 179/1eU
5.00 J/cm²
23.8 ft-lb/in²
conditioned; ISO 179/1eU
3.00 J/cm²

@Temperature 30.0 °C
14.3 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
3.00 J/cm²

@Temperature 30.0 °C
14.3 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
dry; ISO 179/1eA
0.800 J/cm²
3.81 ft-lb/in²
conditioned; ISO 179/1eA
0.300 J/cm²

@Temperature 30.0 °C
1.43 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.300 J/cm²

@Temperature 30.0 °C
1.43 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
16.7 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 110 °C
194 - 230 °F
long term; EMS
180 °C
356 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 70.0 °C
158 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Descriptive Properties Value Comments
Additives Lubricants
Automotive Automotive electr. and electronics, lighting
Powertrain and Chassis
Electricals & Electronics Electrical appliances
Form Granules
Industry & Consumer goods Heating systems
Mechanical Engineering
Power transmission
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Improved friction & wear properties
Special Characteristics Improved heat resistance