Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 532 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
ASTM D648
Quadrant EPP Duratron® PAI T4203 Extruded Polyamide-imide (ASTM Product Data Sheet)
Deflection Temperature at 1.8 MPa (264 psi) 278 °C

@Thickness 3.20 mm
532 °F

@Thickness 0.126 in
Annealed; 2 hours at 200°C; ASTM D648
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-755 SL45 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like the ot..
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
ASTM D648
Quadrant EPP Duratron® PAI T4503 Compression Molded, Polyamide-imide, Eelectrical Grade (ASTM Product Data Sheet)
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
ASTM D648
Quadrant EPP Semitron® CMP XL20 (ASTM Product Data Sheet)
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate particulat..
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon PAI has the hi..
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not only..
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear (Europe-Africa-Middle East)
LNP* Lubricomp* OCL4036L is a compound based on PPS - Linear resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP LUBRICOMP OCL36XXP PPS - Linear (Europe-Africa-Middle East)
LNP* LUBRICOMP* OCL36XXP is a compound based on PPS- Linear resin containing PTFE, Carbon Fiber. Added features include : Internally Lubricated, Electrically Conductive .
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
Annealed; ASTM D648
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica..
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
Unannealed; Flatwise; ISO 75-2/A
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA), 33% Glass Fiber
Amodel® AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e..
Deflection Temperature at 1.8 MPa (264 psi) 278 °C

@Thickness 3.20 mm
532 °F

@Thickness 0.126 in
Annealed; ASTM D648
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)
AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th..
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
Unannealed; ISO 75-2/A
Solvay Specialty Polymers KetaSpire® KT-880 GF15 Polyetheretherketone (PEEK), 15% Glass Fiber
KetaSpire® KT-880 GF15 is a high flow, 15% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpi..
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)
Torlon® 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate partic..
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)
Torlon® 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon® grades. Torlon® PA..
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)
Torlon® 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not ..
Deflection Temperature at 1.8 MPa (264 psi) 278 °C

@Thickness 3.20 mm
532 °F

@Thickness 0.126 in
unannealed; ASTM D 648
SABIC Innovative Plastics LNP Thermocomp LF004 PEEK
LNP THERMOCOMP* LF004 is a compound based on Polyetheretherketone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
ASTM D648
Plenco 6990 Phenolic, Briquette, Transfer Molded
PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco.
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
ASTM D648
Ensinger TECATOR™ TI 5013 Polyamide-imide (PAI)
TECATOR™ is a high performance melt processable polyamideimide that maintains its excellent mechanical and wear properties in temperature environments exceeding 500°F. Stock shapes from Ensinger ..
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
Unannealed; ASTM D648
Solvay Specialty Polymers Torlon® 4203 Polyamide-imide (PAI)  (discontinued **)
Torlon 4203 is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin for extrusion. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon P..
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
Unannealed; ISO 75-2/Af
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee..
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
ASTM D648
Plenco 1581 Polyester, Briquette, Transfer Molded
PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f..
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
Isoflon PAI Polyamideimide
Materials with strong mechanical and electrical performances under high temperatures.Information provided by Isoflon.
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
ASTM D648
Solvay Specialty Polymers Xydar® MG-350 Liquid Crystal Polymer, Mineral and Glass Filled  (discontinued **)<
XYDAR MG-350 Liquid Crystal Polymer (LCP) is a mineral and glass-filled injection molding grade developed specifically for cost-effective performance in applications where a balance of flatness and ..
Deflection Temperature at 1.8 MPa (264 psi) 278 °C
532 °F
Annealed; ASTM D648
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically ..
Copyright © lookpolymers.com All Rights Reserved