Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 86.0 - 370 µm/m-°C @Temperature -40.0 - 85.0 °C |
47.8 - 206 µin/in-°F @Temperature -40.0 - 185 °F |
Average value: 185 µm/m-°C Grade Count:5 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
CTE, linear | 9.00 - 370 µm/m-°C | 5.00 - 206 µin/in-°F | Average value: 66.6 µm/m-°C Grade Count:8 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |