Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 86.0 µm/m-°C @Thickness 2.00 mm, Temperature -125 - 20.0 °C |
47.8 µin/in-°F @Thickness 0.0787 in, Temperature -193 - 68.0 °F |
ASTM E831-06 |
NeXolve UV Blocking Optionox® Polyimide Film/Coating Highly UV durable with excellent weatherability and stability to ozone.Optinox® films and coatings are highly UV durable and exhibit excellent weathering durability, including very high stability .. |
|||
CTE, linear | 86.0 - 370 µm/m-°C @Temperature -40.0 - 85.0 °C |
47.8 - 206 µin/in-°F @Temperature -40.0 - 185 °F |
Average value: 185 µm/m-°C Grade Count:5 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
CTE, linear | 86.0 µm/m-°C @Temperature 20.0 °C |
47.8 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
BASF Capron® 8224 HSL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
CTE, linear | 86.0 µm/m-°C @Temperature 20.0 °C |
47.8 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
LG Chemical AF-320T ABS, Flame Retardant, High Impact, High Flow, Slim Wall Information Provided by LG Chem |
|||
CTE, linear | 86.0 µm/m-°C @Temperature 40.0 - 130 °C |
47.8 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 1586 Polyester, Pellet, Injection Molded PLENCO 01586 is a glass and mineral reinforced pelletized polyester molding compound offering excellent heat resistance and mechanical strength properties. This product is typically used for injecti.. |
|||
CTE, linear | 86.0 µm/m-°C | 47.8 µin/in-°F | Above Tg |
Tra-Con Tra-Bond 77-2LTC Low Temperature Cure SMD Adhesive TRA-BOND 77-2LTC one component, solvent-free, insulative epoxy adhesive is designed to cure at temperatures as low as 80°C. This adhesive is specifically designed for attaching surface mounted devi.. |
|||
CTE, linear | 86.0 µm/m-°C @Temperature 20.0 °C |
47.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Devcon Plastic Steel® Putty (A) Epoxy General Repair EpoxyComments: The original metal-filled epoxy putty used for hundreds of routine maintenance, production and tooling applications. Bonds to most metal, concrete and some plastics. .. |
|||
CTE, linear | 86.0 µm/m-°C @Temperature 20.0 °C |
47.8 µin/in-°F @Temperature 68.0 °F |
|
Armstrong A-2/W Epoxy Adhesive This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac.. |
|||
CTE, linear | 86.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
47.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359 |
CENTROPLAST CENTROLAB HT Polypropylene Higher Temperatures PP-HT is a semi-crystalline plastic, with high acid and chemical resistance and mechanical strength. Due to its high resistance to temperature, PP-HT-plastics are often used in medical technology as.. |