Thermal Properties Metric English Comments
CTE, linear 86.0 - 370 µm/m-°C

@Temperature -40.0 - 85.0 °C
47.8 - 206 µin/in-°F

@Temperature -40.0 - 185 °F
Average value: 185 µm/m-°C Grade Count:5
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m..
CTE, linear 9.00 - 370 µm/m-°C
5.00 - 206 µin/in-°F
Average value: 66.6 µm/m-°C Grade Count:8
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%..