Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

North Wood Plastics Polypropylene with 20% Wood Fiber, Extrusion Grade

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Wood Filled
Manufacturer North Wood Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF North Wood Plastics Polypropylene with 20% Wood Fiber, Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by North Wood Plastics, Inc.
Physical Properties Metric English Comments
Density 0.951 g/cc
0.0344 lb/in³
ASTM D792
Melt Flow <= 0.50 g/10 min

@Temperature 190 °C
<= 0.50 g/10 min

@Temperature 374 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.0 MPa
4640 psi
ASTM D638
Tensile Modulus 2.70 GPa
392 ksi
ASTM D638
Flexural Yield Strength 56.0 MPa
8120 psi
ASTM D790
Flexural Modulus 2.50 GPa
363 ksi
ASTM D790
Izod Impact, Notched 0.460 J/cm
0.862 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.00 J/cm
3.75 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 63.0 µm/m-°C

@Temperature 20.0 °C
35.0 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature <= 200 °C
<= 392 °F
To prevent fiber degradation.