Thermal Properties Metric English Comments
CTE, linear 57.6 µm/m-°C
32.0 µin/in-°F
ASTM E831
SABIC Innovative Plastics Lexan® FR66 Polycarbonate Film, Flame Retardant
Lexan FR66 flame-retardant film is a clear, thin-gauge polycarbonate film with a suede finish on one side and a matte finish on the other, and a UL94 V-0 listing to meet the stringent requirements i..
CTE, linear 57.6 µm/m-°C
32.0 µin/in-°F
ASTM E831
SABIC Innovative Plastics Lexan® FR700 Polycarbonate Film, Flame Retardant
Lexan FR700 is a black, one side fine matt, one side velvet flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good d..
CTE, linear 57.6 µm/m-°C
32.0 µin/in-°F
ASTM E831
SABIC Innovative Plastics Lexan® FR83 Polycarbonate Film, Flame Retardant
Lexan* FR83 flame-retardant film is a matt/polished, thin-gauge polycarbonate film with a UL94 VTM-0 listing to meet the stringent requirements in a wide range of electrical, electronic and transpor..
CTE, linear 57.6 µm/m-°C
32.0 µin/in-°F
ASTM E831
SABIC Innovative Plastics Lexan® FR60 Polycarbonate Film, Flame Retardant
Lexan FR60 flame-retardant film is a clear, thin-gauge polycarbonate film with polished surfaces on both sides, and a UL94 V-0 listing to meet the stringent requirements in a wide range of electrica..
CTE, linear 57.6 µm/m-°C
32.0 µin/in-°F
ASTM E831
SABIC Innovative Plastics Lexan® FR63 Polycarbonate Film, Flame Retardant
Lexan FR63 flame-retardant film is a clear, thin-gauge polycarbonate film with a matte finish on one side and a polish finish on the other and a UL94 V-0 listing to meet the stringent requirements i..
CTE, linear 57.6 µm/m-°C
32.0 µin/in-°F
ASTM E831
SABIC Innovative Plastics Lexan® FR735A Polycarbonate Film, Flame Retardant
Lexan FR735A is a black, one side velvet, one polish flame-retardant polycarbonate film with a UL94 V-0 listing at 0.250 mm. This film has formability, excellent mechanical properties, good dimensio..
CTE, linear 57.6 µm/m-°C

@Temperature -30.0 - 100 °C
32.0 µin/in-°F

@Temperature -22.0 - 212 °F
Inchem Phenoxy PKFE
Phenoxy PKFE - polyhydroxy ether of Bisphenol A. Originally developed by Union Carbide. Produced by InChem Corporation.
CTE, linear 57.6 µm/m-°C

@Temperature 20.0 °C
32.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
ITW Devcon Metal Repair Wear Resistant Epoxy (WR-2), Dark Grey
Information provided by ITW Devcon
CTE, linear 57.6 µm/m-°C

@Temperature 20.0 °C
32.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech PETG 3D Lenticular 3-D Specialty Sheet
Description: Specialty SheetInformation provided by Spartech.
CTE, linear 57.6 µm/m-°C

@Temperature 20.0 °C
32.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Lubrizol ISOPLAST™ 302EZ Engineering Thermoplastic Polyurethane Resin
NSF Standard 61 CertifiedInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
CTE, linear 57.6 µm/m-°C

@Temperature 20.0 °C
32.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
CPC - Vycom CELTEC MARINE™ Expanded Foam PVC Polyvinyl Chloride
Celtec Marine is made from rigid expanded foam polyvinyl chloride (PVC) material whose combination of features makes it ideal for wood trim and plywood replacement in boat manufacturing. Its closed ..
CTE, linear 57.6 µm/m-°C

@Temperature 20.0 °C
32.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
CPC - Vycom VINTEC I® PVC Polyvinyl Chloride (PVC)
Vintec I is a normal impact, high corrosion resistant polyvinyl chloride (PVC) sheet. Because of its exceptional corrosion resistance, it is ideally suited for applications where maximum chemical re..
CTE, linear 57.6 µm/m-°C
32.0 µin/in-°F
ASTM E831
Ensinger Tecatron® XP-61L Compression Molded PPS Compound, 25% Fiberglass and Mineral Filled
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p..
CTE, linear 57.6 µm/m-°C
32.0 µin/in-°F
CMT Materials HYTAC® XTL Tough Thermoplastic Syntactic Foam
HYTAC®-XTL was developed to offer an improved surface quality after machining when compared to our popular HYTAC-B1X. This is particularly important when working with sticky or transparent plastic..
CTE, linear 57.6 µm/m-°C

@Temperature 20.0 °C
32.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Axiall ProTherm® 4345 Rigid PVC, Extrusion
Georgia Gulf ProTherm® 4345 is a CPVC powder blend designed for extrusion applications requiring high heat deflection temperatures. Processing and stability along with overall physical properties ..
CTE, linear 57.6 µm/m-°C

@Temperature 20.0 °C
32.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Asahi Kasei Thermofil D-10FG-1101 10% Glass Fiber Reinforced, ABS
Information provided by Asahi Thermofil
CTE, linear 57.6 µm/m-°C
32.0 µin/in-°F
BCC Products BC 7053 Epoxy Casting
BC 7053 is an iron filled epoxy casting system. This system is a high iron content material that provides unsurpassed wear resistance. BC7053 was designed for use in constructing core boxes, holding..
CTE, linear 57.6 µm/m-°C
32.0 µin/in-°F
BCC Products BC 7062H Epoxy Casting
BC 7062 are aluminum filled, low viscosity epoxy mass casting resins. These room temperature cure systems allow the user choice thicknesses of 1/8 inch to a maximum of 6 inches without foaming or yi..
CTE, linear 57.6 µm/m-°C

@Temperature 20.0 °C
32.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
CPC - Vycom Ultra White™ PVC Advanced, UV (Ultra Violet) resistant sheet
Ultra White is an advanced PVC formulation designed specifically for outdoor applications where resistance to ultraviolet (UV) degradation is critical. Tests show that Ultra White retards both surfa..
CTE, linear 57.6 µm/m-°C
32.0 µin/in-°F
ASTM E831
SABIC Innovative Plastics Lexan® FR65 Polycarbonate Film, Flame Retardant
Lexan FR65 flame-retardant film is a clear, thin-gauge polycarbonate film with a velvet finish on one side and a matt finish on the other, and a UL94 V-0 listing to meet the stringent requirements i..
CTE, linear 57.6 µm/m-°C

@Temperature 20.0 °C
32.0 µin/in-°F

@Temperature 68.0 °F
ASTM D1525
PlastxWorld CEVIAN® S5210 10% GF PC/ABS alloy
Glass fiber reinforced and flame retarded PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld ..
CTE, linear 57.6 µm/m-°C

@Temperature 20.0 °C
32.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Spartech APET SP4110 Copolyester Sheet
Description: Copolyester SheetInformation provided by Spartech.