Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis BorPEX™ HE2557 Yellow High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide))

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer Borealis
Trade Name BorPEX™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BorPEX™ HE2557 Yellow High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide)).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BorPEX HE2557 is a yellow, high molecular weight, high density polyethylene compound for crosslinkable pipes, specially designed for peroxide crosslinking. Long term stability and UV resistance is ensured by an optimized stabilization system. Crosslinked pipes made from BorPEX HE2557 are recommended for natural gas and industrial applications.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
Base Resin; ISO 1183
0.958 g/cc
0.0346 lb/in³
Compound; ISO 1183
High Load Melt Index 6.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
6.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 210 °C
410 °F
50 Minutes; EN 728
Users viewing this material also viewed the following: