Menzolit Menzolit® BMC 0190 Unsaturated Polyester UP

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer Menzolit
Trade Name Menzolit®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Menzolit Menzolit® BMC 0190 Unsaturated Polyester UP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC 0190 is a general purpose BMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The flammability meets the demands of standard UL 94 category V0. For grey tones, a certificate (yellow-card) is available on request. The glass content is on a level that combines good mouldability with good mechanical properties regarding strength and stiffness.Information Provided by Menzolit
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
ISO 1183
Water Absorption <= 0.50 %
<= 0.50 %
ISO 62
Linear Mold Shrinkage 0.0015 cm/cm
0.0015 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 31.0 MPa

@Temperature 22.0 °C
4500 psi

@Temperature 71.6 °F
25mm flat samples, compression moulded; ISO 527-4
Tensile Strength, Yield 31.0 MPa

@Temperature 22.0 °C
4500 psi

@Temperature 71.6 °F
25mm flat samples, compression moulded; ISO 527-4
Elongation at Yield 0.00 %
0.00 %
tensile rupture strain; ISO 527-4
Modulus of Elasticity 13.0 GPa
1890 ksi
25mm flat samples, compression moulded; ISO 527-4
Flexural Strength 99.0 MPa

@Temperature 22.0 °C
14400 psi

@Temperature 71.6 °F
25 mm wide 100 mm long, flat samples; ISO 14125
Flexural Modulus 10.0 GPa

@Temperature 22.0 °C
1450 ksi

@Temperature 71.6 °F
25 mm wide 100 mm long, flat samples; ISO 14125
Poissons Ratio 0.30
0.30
Shear Modulus 5.00 GPa
725 ksi
in plane
Charpy Impact, Notched 2.90 J/cm²
13.8 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear 10.0 µm/m-°C
5.56 µin/in-°F
ISO 11359-2
Specific Heat Capacity 1.10 J/g-°C
0.263 BTU/lb-°F
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 165 °C
329 °F
Deflection Temperature at 1.8 MPa (264 psi) >= 130 °C
>= 266 °F
ISO 75-2
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Glass Transition Temp, Tg 170 °C
338 °F
ISO 11357-2
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Oxygen Index 30 %
30 %
ISO 4589-2
Glow Wire Test 960 °C
1760 °F
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 4.0
4.0
IEC 60250
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60243-1
Dissipation Factor 0.010
0.010
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Processing Properties Metric English Comments
Processing Temperature 135 - 150 °C
275 - 302 °F
Injection moulding, matched metal die