Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed 1950°F (1070°C)

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Special Metals (includes the former Inco Alloys International Inc.)
Trade Name INCONEL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Special Metals INCONEL® 625LCF® Nickel Superalloy (UNS N06626) Annealed 1950°F (1070°C).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tensile strength (ultimate and yield), elongation, and hardness values are for samples annealed 1950°F (1070°C)/5 minutes/AC. This produces ASTM grain size 9.5. Other property values are typical of this alloy.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.44 g/cc
0.305 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 96
96
Tensile Strength, Ultimate 957.0 MPa
138800 psi
Tensile Strength, Yield 535 MPa

@Strain 0.200 %
77600 psi

@Strain 0.200 %
Elongation at Break 45 %
45 %
Modulus of Elasticity 208 GPa
30200 ksi
Poissons Ratio 0.28
0.28
Shear Modulus 81.4 GPa
11800 ksi
Thermal Properties Metric English Comments
CTE, linear 12.8 µm/m-°C

@Temperature 21.0 - 100 °C
7.11 µin/in-°F

@Temperature 69.8 - 212 °F
Mean
13.3 µm/m-°C

@Temperature 21.0 - 300 °C
7.39 µin/in-°F

@Temperature 69.8 - 572 °F
Mean
13.9 µm/m-°C

@Temperature 21.0 - 500 °C
7.72 µin/in-°F

@Temperature 69.8 - 932 °F
Mean
14.9 µm/m-°C

@Temperature 21.0 - 700 °C
8.28 µin/in-°F

@Temperature 69.8 - 1290 °F
Mean
Specific Heat Capacity 0.410 J/g-°C
0.0980 BTU/lb-°F
Thermal Conductivity 9.70 W/m-K
67.3 BTU-in/hr-ft²-°F
Melting Point 1290 - 1350 °C
2350 - 2460 °F
Solidus 1290 °C
2350 °F
Liquidus 1350 °C
2460 °F
Maximum Service Temperature, Air 650 °C
1200 °F
resistance to low cycle and thermal fatigue
Component Elements Properties Metric English Comments
Aluminum, Al <= 0.40 %
<= 0.40 %
Carbon, C <= 0.030 %
<= 0.030 %
Chromium, Cr 20 - 23 %
20 - 23 %
Cobalt, Co <= 1.0 %
<= 1.0 %
Iron, Fe <= 5.0 %
<= 5.0 %
Manganese, Mn <= 0.50 %
<= 0.50 %
Molybdenum, Mo 8.0 - 10 %
8.0 - 10 %
Nickel, Ni >= 58 %
>= 58 %
Niobium, Nb (Columbium, Cb) 3.15 - 4.15 %
3.15 - 4.15 %
Includes Ta
Nitrogen, N <= 0.020 %
<= 0.020 %
Phosphorous, P <= 0.015 %
<= 0.015 %
Silicon, Si <= 0.020 %
<= 0.020 %
Sulfur, S <= 0.015 %
<= 0.015 %
Titanium, Ti <= 0.40 %
<= 0.40 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000132 ohm-cm
0.000132 ohm-cm
Magnetic Permeability 1.0006
1.0006
at 200 Oersted (15.9 kA/m)
Users viewing this material also viewed the following: