Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 42.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® NX07353 PC+ABS (Asia Pacific)
Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications.
CTE, linear, Parallel to Flow 42.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® NX07353 PC+ABS (Asia Pacific)
Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications.
CTE, linear, Parallel to Flow 42.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® RCM6123 PC+ABS (Asia Pacific)
Cycoloy* RCM6123 resin is an injection moldable filled PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 rating @ 1..
CTE, linear, Parallel to Flow 42.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® C7230P PC+ABS (Asia Pacific)
Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications.
CTE, linear, Parallel to Flow 42.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Cycoloy® C7230P PC+ABS (Asia Pacific)
Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications.
CTE, linear, Parallel to Flow 42.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66
LNP* LUBRICOMP* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
CTE, linear, Parallel to Flow 42.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66 (Asia Pacific)
LNP* Lubricomp* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 42.0 µm/m-°C

@Temperature 23.0 - 150 °C
23.3 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Valox® ENH4530 PBT (Europe-Africa-Middle East)
15% GF PBT, Non-Brominated & Non-Chlorinated Flame retardant
CTE, linear, Parallel to Flow 41.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP DF004ER PC
LNP THERMOCOMP* DF004ER is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. Mold Release.
CTE, linear, Parallel to Flow 42.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI
LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
CTE, linear, Parallel to Flow 42.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI (Asia Pacific)
LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
CTE, linear, Parallel to Flow 42.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP PH0460A PA 6
LNP* THERMOCOMP* PH0460A is a compound based on Nylon 6. Added feature of this material is: High Specific Gravity.
CTE, linear, Parallel to Flow 42.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl GTX GTX965 PPE+PA66
NORYL GTX965 is a mineral reinforced PPE/PA blend. It offers excellent surface appearance, processability and dimensional stability at elevated temperatures. The best molding condition for good appe..
CTE, linear, Parallel to Flow 42.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East)
Super high flow FR PBT grade with 15% Glass reinforced
CTE, linear, Parallel to Flow 42.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL GTX GTX675 PPE+PA6
Noryl GTX* GTX675 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to a..
CTE, linear, Parallel to Flow 42.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP PH0460A PA 6 (Asia Pacific)
LNP* Thermocomp* PH0460A is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
CTE, linear, Parallel to Flow 41.9 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East)
VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin.
Copyright © lookpolymers.com All Rights Reserved