Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 82.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP FARADEX WX94736 PBT
LNP* Faradex* WX94736 is a compound based on Polybutylene Terephalate resin containing Stainless Steel.
CTE, linear, Parallel to Flow 82.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66
LNP* LUBRICOMP* RFL33 is a compound based on Nylon 66 resin containing 15% Glass Fiber, 15% PTFE. Added feature of this material is: Wear Resistant.
CTE, linear, Parallel to Flow 82.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 (Asia Pacific)
LNP* Lubricomp* RFL33 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 82.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP RX01514 PA 66
LNP* LUBRICOMP* RX01514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
CTE, linear, Parallel to Flow 82.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP RX01514 PA 66 (Asia Pacific)
LNP* Lubricomp* RX01514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
CTE, linear, Parallel to Flow 82.8 µm/m-°C

@Temperature 60.0 - 138 °C
46.0 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 365 PC+PET
Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031"".
CTE, linear, Parallel to Flow 82.8 µm/m-°C

@Temperature 60.0 - 138 °C
46.0 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 365 PET (Asia Pacific)
Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031"".
CTE, linear, Parallel to Flow 82.8 µm/m-°C

@Temperature -40.0 - 95.0 °C
46.0 µin/in-°F

@Temperature -40.0 - 203 °F
ASTM E 831
SABIC Innovative Plastics Xenoy® 1731 PBT+PC
Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.
CTE, linear, Parallel to Flow 82.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer
LNP* THERMOCOMP* KF006XXC is a compound based on Acetal Copolymer resin containing 30% Glass Fiber.
CTE, linear, Parallel to Flow 82.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer (Asia Pacific)
LNP* Thermocomp* KF006XXC is a compound based on Acetal Copolymer resin containing Glass Fiber.
CTE, linear, Parallel to Flow 82.8 µm/m-°C

@Temperature 60.0 - 138 °C
46.0 µin/in-°F

@Temperature 140 - 280 °F
ASTM E 831
SABIC Innovative Plastics Valox® 365 PET
Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031".This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 82.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON RE002 PA 66
LNP* STAT-KON* RE002 is a compound based on Nylon 66 resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Parallel to Flow 82.8 µm/m-°C

@Temperature -40.0 - 40.0 °C
46.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON RE002 PA 66 (Asia Pacific)
LNP* Stat-kon* RE002 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.