Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 188 °C | 370 °F | Zone 3 |
Premix Thermoplastics PRE-ELEC® ESD 7100 PRE-ELEC ESD 7100 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7100 has been developed for inject.. |
|||
Die Temperature | 188 °C | 370 °F | Zone 5 |
Premix Thermoplastics PRE-ELEC® ESD 7120 PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject.. |
|||
Die Temperature | 188 °C | 370 °F | Zone 2 |
Premix Thermoplastics PRE-ELEC® ESD 7120 PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject.. |
|||
Die Temperature | 188 °C | 370 °F | Zone 3 |
Premix Thermoplastics PRE-ELEC® ESD 7120 PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject.. |
|||
Die Temperature | 188 °C | 370 °F | Zone 4 |
Premix Thermoplastics PRE-ELEC® ESD 7120 PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject.. |
|||
Die Temperature | 188 °C | 370 °F | Zone 1 |
Premix Thermoplastics PRE-ELEC® ESD 7120 PRE-ELEC ESD 7120 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7120 has been developed for inject.. |
|||
Die Temperature | 188 °C | 370 °F | Zone 3 |
Premix Thermoplastics PRE-ELEC® ESD 7200 PRE-ELEC ESD 7200 is a static dissipative thermoplastic compound based on PC/ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7200 has been developed for inj.. |
|||
Die Temperature | 188 °C | 370 °F | Zone 4 |
Premix Thermoplastics PRE-ELEC® ESD 1100
(discontinued **) PRE-ELEC ESD 1100 is a static dissipative thermoplastic compound based on PETG. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 1100 has been developed for the e.. |
|||
Die Temperature | 188 °C | 370 °F | Zone 1 |
Premix Thermoplastics PRE-ELEC® ESD 1100
(discontinued **) PRE-ELEC ESD 1100 is a static dissipative thermoplastic compound based on PETG. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 1100 has been developed for the e.. |
|||
Die Temperature | 188 °C | 370 °F | Zone 2 |
Premix Thermoplastics PRE-ELEC® ESD 1100
(discontinued **) PRE-ELEC ESD 1100 is a static dissipative thermoplastic compound based on PETG. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 1100 has been developed for the e.. |
|||
Die Temperature | 188 °C | 370 °F | Zone 5 |
Premix Thermoplastics PRE-ELEC® ESD 1100
(discontinued **) PRE-ELEC ESD 1100 is a static dissipative thermoplastic compound based on PETG. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 1100 has been developed for the e.. |
|||
Die Temperature | 188 °C | 370 °F | Zone 2, Extrusion |
Lubrizol ESTANE® 58244 Ether Based Thermoplastic Polyurethane Features: Non-Halogenated flame retardant compoundUses: Extrusion – wire and cable and general extrusion where flame retardant propertied are requiredAvailable in Americas, Europe, Middle East, Afr.. |
|||
Die Temperature | 188 °C | 370 °F | Zone 2, Extrusion |
Lubrizol ESTANE® 58370 Ether Based Thermoplastic Polyurethane Features: Halogenated flame retardant compoundUses: Extrusion – Wire and cable and general application where flame retardant properties are neededAvailable in Americas, Europe, Middle East, Africa,.. |
|||
Die Temperature | 188 °C | 370 °F | Zone 1, 6, Extrusion |
Lubrizol ESTANE® 54610 Ester Based Thermoplastic Polyurethane Features: Good physical properties and chemical resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusion.Available in Americas, Europe, Midd.. |
|||
Die Temperature | 188 °C | 370 °F | Zone 2, Extrusion |
Lubrizol ESTANE® 54610 Ester Based Thermoplastic Polyurethane Features: Good physical properties and chemical resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusion.Available in Americas, Europe, Midd.. |
|||
Die Temperature | 188 °C | 370 °F | Zone 1, Extrusion |
Lubrizol ESTANE® 54640 Ether Based Thermoplastic Polyurethane Very good physical properties and hydrolysis resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusionAvailable in Americas, Europe, Middle E.. |
|||
Die Temperature | 188 °C | 370 °F | Zone 2, Extrusion |
Lubrizol ESTANE® 54640 Ether Based Thermoplastic Polyurethane Very good physical properties and hydrolysis resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusionAvailable in Americas, Europe, Middle E.. |
|||
Die Temperature | 188 °C | 370 °F | 6, Zone 1, Extrusion |
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection.. |
|||
Die Temperature | 188 °C | 370 °F | Zone 2, Extrusion |
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection.. |
|||
Die Temperature | 188 °C | 370 °F | Zone 1, 6, Extrusion |
Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane Features: Halogenated flame retardant compound with good low temperature properties and cut resistanceUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant properti.. |
|||
Die Temperature | 188 °C | 370 °F | Zone 2, Extrusion |
Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane Features: Halogenated flame retardant compound with good low temperature properties and cut resistanceUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant properti.. |
|||
Die Temperature | 188 °C | 370 °F | Zone 1, Extrusion |
Lubrizol ESTANE® 58311 Ether Based Thermoplastic Polyurethane Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Flat Die/Cast Film Extrusion, Profile ExtrusionAv.. |
|||
Die Temperature | 188 °C | 370 °F | Zone 2, Extrusion |
Lubrizol ESTANE® 58311 Ether Based Thermoplastic Polyurethane Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Flat Die/Cast Film Extrusion, Profile ExtrusionAv.. |