Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 371 °C | 700 °F | |
Oxford Polymers PEEK 20GF-Natural PEEK, 20% Glass Fiber Reinforced Product Description: Glass Fiber (20% Reinforced), PEEK, Polyetheretherketone injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Glass fiber Special Chara.. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better dimensiona.. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 resin. .. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of.. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stability.. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gr.. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gra.. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.In.. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Middle Barrel Temperature | 371 - 421 °C | 700 - 790 °F | |
LNP ULTEM® EXCP0096 Polyetherimide, 30% Carbon Fiber Reinforcement, 10% PTFE Lubricant
(discontinued **) Features: Lubricated, Electrically Conductive, Good Wear Resistance, High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This dat.. |
|||
Middle Barrel Temperature | 371 - 421 °C | 700 - 790 °F | |
LNP ULTEM® UC3000 Polyetherimide, 30% Carbon Fiber Reinforcement
(discontinued **) High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo.. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621.. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r.. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better di.. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 res.. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining.. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers AvaSpire® AV-848 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-848 CF30 is a 30% carbon fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparabl.. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable.. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK) AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stabi.. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers KetaSpire® KT-820 GF15 Polyetheretherketone (PEEK), 15% Glass Fiber KetaSpire® KT-820 GF15 is a low flow, 15% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpir.. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers KetaSpire® KT-820 SL45 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provide.. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers KetaSpire® KT-880 GF15 Polyetheretherketone (PEEK), 15% Glass Fiber KetaSpire® KT-880 GF15 is a high flow, 15% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpi.. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers KetaSpire® KT-880 GF20 Polyetheretherketone (PEEK), 20% Glass Fiber KetaSpire® KT-880 GF20 is a high flow, 20% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpi.. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |
|||
Middle Barrel Temperature | 371 °C | 700 °F | |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This resin ret.. |
|||
Middle Barrel Temperature | 371 - 393 °C | 700 - 739 °F | |
LNP ULTEM® SMU5806 Polyetherimide, 8% Carbon Fiber Reinforcement
(discontinued **) Features: Low ShrinkageForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still.. |
|||
Middle Barrel Temperature | 371 - 421 °C | 700 - 790 °F | |
LNP ULTEM® SMU5832 Polyetherimide, 30% CarbonGlassMineral Reinforced
(discontinued **) ESD characteristics for ultra high-heat applications. Will be UC3010.Features: High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Compan.. |
|||
Middle Barrel Temperature | 371 - 421 °C | 700 - 790 °F | |
LNP ULTEM® SMU5852 Polyetherimide, 30% Carbon Fiber Reinforcement, 15% PTFE Lubricant
(discontinued **) Features: Lubricated, Electrically Conductive, Good Wear ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Dis.. |
|||
Middle Barrel Temperature | 371 - 421 °C | 700 - 790 °F | |
LNP ULTEM® SMU5834 Polyetherimide, 20% Carbon Fiber Reinforcement
(discontinued **) High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo.. |
|||
Middle Barrel Temperature | 371 - 421 °C | 700 - 790 °F | |
LNP ULTEM® SMU5836 Polyetherimide, 30% Carbon Fiber Reinforcement
(discontinued **) High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo.. |