Material Notes:
Description: Unreinforced polyamide PA6, high viscosity, with high flexibility and very high impact resistance even at low temperature, for extrusion.Available in: Europe Product Applications: It has high flexibility and very high impact strength. It is specially available for pipes extrusion.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183/A
Water Absorption 1.15 %

@Temperature 23.0 °C,
Time 86400 sec
1.15 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
ISO 527 type 1 A
Elongation at Break 220 %
220 %
ISO 527 Type 1A
Tensile Modulus 0.900 GPa
131 ksi
ISO 527 Type 1A
Flexural Strength 40.0 MPa
5800 psi
ISO 178
Flexural Modulus 0.850 GPa
123 ksi
ISO 178
Izod Impact, Notched (ISO) 85.0 kJ/m²
40.4 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched NB
NB
ISO 179/1eU
Charpy Impact, Notched NB
NB
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C

@Temperature 23.0 - 85.0 °C
38.9 µin/in-°F

@Temperature 73.4 - 185 °F
ISO 11359
Melting Point 222 °C
432 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75/Af
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 3.7
3.7
IEC 60250
Dissipation Factor 0.020
0.020
IEC 60250
Processing Properties Metric English Comments
Feed Temperature 200 - 210 °C
392 - 410 °F
Front Barrel Temperature 210 - 220 °C
410 - 428 °F
Die Temperature 220 - 230 °C
428 - 446 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 210-220°C