Processing Properties Metric English Comments
Front Barrel Temperature 230 °C
446 °F
Inchem Phenoxy PKFE
Phenoxy PKFE - polyhydroxy ether of Bisphenol A. Originally developed by Union Carbide. Produced by InChem Corporation.
Front Barrel Temperature 230 - 250 °C
446 - 482 °F
Injection Molding
LG Chemical KEYFLEX BT 3047D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Front Barrel Temperature 230 - 250 °C
446 - 482 °F
Injection Molding
LG Chemical LUCON 6080EX ABS+CF
Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Wide Processing RangeApplication: Carrying Cart Pipe Coating, BLU carrying TrayCAS No. 9003-56-9, 9003-54-7 and 7782-42-6Informatio..
Front Barrel Temperature 230 - 250 °C
446 - 482 °F
LG Chemical LUMAX HF-5006F High Flow PBT, Weather Resistant, Flame Retardant
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
Front Barrel Temperature 230 - 250 °C
446 - 482 °F
LG Chemical LUMAX IN-5001 High Impact PBT
LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r..
Front Barrel Temperature 230 - 250 °C
446 - 482 °F
LG Chemical LUPOS HR-2207 Heat Resistant SAN, 20% Glass Fiber Reinforced
LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have ..
Front Barrel Temperature 230 - 250 °C
446 - 482 °F
LG Chemical LUPOS HR-2307 Heat Resistant SAN, 30% Glass Fiber Reinforced
LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have ..
Front Barrel Temperature 230 - 250 °C
446 - 482 °F
Injection Molding
LG Chemical XR409E ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch..
Front Barrel Temperature 230 - 240 °C
446 - 464 °F
Injection Molding
LG Chemical XR409HJ ABS, Heat Resistance, Curl Fit
Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior & Exterior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by ..
Front Barrel Temperature 230 - 250 °C
446 - 482 °F
Injection Molding
LG Chemical XR419 ABS, Heat Resistance, Chemical Resistance
Feature: Injection Molding, Heat Resistance, Chemical ResistanceApplication: Automotives Interior Housing (Ventgrille Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provide..
Front Barrel Temperature 230 - 250 °C
446 - 482 °F
Injection Molding
LG Chemical XR474 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior HousingCAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical
Front Barrel Temperature 230 - 260 °C
446 - 500 °F
Gromax 1163LL TPE
163LL is medium modulus grade with nominal Durometer hardness of 63D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ext..
Front Barrel Temperature 230 - 260 °C
446 - 500 °F
Start Point: 240°C
Kingfa MAC-701 PC/ABS Alloy
Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic p..
Front Barrel Temperature 230 - 240 °C
446 - 464 °F
Injection Molding
LG Chemical ER461 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica..
Front Barrel Temperature 230 - 240 °C
446 - 464 °F
Injection Molding
LG Chemical XR401 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (lamp housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 ..
Front Barrel Temperature 230 - 240 °C
446 - 464 °F
Solvay Technyl® C 206 Nylon 6, EH0
Unreinforced Plyamide PA6, standard for fast cycling, for injection molding.Technyl C 206 has high fluidity and good mold release, favored by a high crystallization rate. It is specially suitable f..
Front Barrel Temperature 230 - 240 °C
446 - 464 °F
Solvay TECHNYL® C 206 PA6, DRY
Description: Unreinforced Polyamide PA6, standard for fast cycling, for injection molding.Available in: EuropeProduct Applications: TECHNYL® C 206 has fluidity and a good mould release, favored b..
Front Barrel Temperature 230 - 235 °C
446 - 455 °F
Solvay TECHNYL® C 246 M PA6, DRY
Description: Unreinforced polyamide 6, with high impact resistance, for injection molding. Grade formerly known as PSB196.Available in: EuropeProduct Applications: It is particularly adapted to the ..
Front Barrel Temperature 230 - 240 °C
446 - 464 °F
Solvay TECHNYL® C 246 V 30 PA6, 30% glass fiber, DRY
Description: Polyamide PA6, reinforced with 30 % of glass fiber, high impact strength, for injection molding.Available in: Asia Pacific and North AmericaProduct Applications: Having good mechanical ..
Front Barrel Temperature 230 °C
446 °F
Solvay TECHNYL® C 507XT PA6, DRY
Description: Unreinforced polyamide 6, heat stabilized, very high viscosity, for extrusion.Available in: Europe Product Applications: It is suitable for extruded semi-finished products, such as: Rod..
Front Barrel Temperature 230 - 240 °C
446 - 464 °F
Solvay Technyl® C206F Unfilled, Fast Cycle Nylon 6
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Front Barrel Temperature 230 - 250 °C
446 - 482 °F
Samsung Cheil Industries Starex® SR-0300 Heat Resistant Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 230 - 250 °C
446 - 482 °F
H3
Samsung Cheil Industries Starex® WR-9330I Heat Resistant Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 230 - 280 °C
446 - 536 °F
Teknor Apex Beetle® 60GS6 Nylon 6, 30% Glass Bead Reinforced, Dry
Features: High rigidity and low warping. Processing Method: Injection MoldingForms: Pellets Injection Notes: Drying is necessary if material has been exposed to air for longer than 3 hours; Back Pr..
Front Barrel Temperature 230 - 280 °C
446 - 536 °F
Teknor Apex Beetle® MDF50 Nylon 6, 50% Short Glass Fiber Filler
Notes: MDF50 is a 50% glass fiber reinforced nylon 6 that offers excellent mechanical performance coupled with good surface finish Features: Good Surface FinishProcessing Method: Injection molding F..
Front Barrel Temperature 230 - 250 °C
446 - 482 °F
Samsung Cheil Industries Starex® SR-0310 Heat Resistant Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature >= 230 °C
>= 446 °F
Borealis Daploy™ SF203HMS High Melt Strength Polypropylene for Extrusion Coating
Daploy SF203HMS resin is a statistic-heterophasic-propylene-ethylene copolymer modified with a polypropylene based structurally isomeric polymer which combines a significantly increased melt strengt..
Front Barrel Temperature 230 - 250 °C
446 - 482 °F
Injection Molding
LG Chemical KEYFLEX BT S5035 Ester Type TPE