Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 270 - 280 °C | 518 - 536 °F | |
NHEP Spectron™ E6126 Nylon 66, 20% Glass Fiber Natural color. E6126 exhibits high rigidity, mechanical strength, and excellent appearance. It is suitable for wide range of applications.Property data measured at room temperature, 50% RH.Informati.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Start Point: 265°C |
Kingfa PA6-G50 50% Glass Fiber Reinforced PA6 Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Start Point: 265°C |
Kingfa PA6-MG30 30% Glass & Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Front Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
LG Chemical LUMID HI1102A(W) PA6, High Impact Feature: Injection Molding, PA6, High ImpactApplication: H/Lamp Screw MountingCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Front Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
LG Chemical LUMID HI1102B(W) PA66, High Impact Feature: Injection Molding,PA66, High ImpactApplication: Automotive (Covers)CAS No. 32131-17-2 and 9010-79-1Information provided by LG Chemical |
|||
Front Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
LG Chemical LUMID HI1202A(W) PA6, High Impact Feature: Injection Molding, PA6, High ImpactApplication: Electric/Electronic PartsCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Front Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
LG Chemical LUMID HI1202B(W) PA66, High Impact Feature: Injection Molding, PA66, High ImpactApplication: Automotive (Covers)CAS No. 32131-17-2 and 9010-79-1Information provided by LG Chemical |
|||
Front Barrel Temperature | 240 - 280 °C | 464 - 536 °F | |
LG Chemical LUPOY HF-5000 High Flow PC/ABS Alloy, Unreinforced Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Front Barrel Temperature | 265 - 280 °C | 509 - 536 °F | Injection Molding |
LG Chemical LUPOY SC5004T PC/Polyester, Transparency Description: Injection Molding, PC/Polyester, General Purpose, Transparency, High FlowApplication: Keypad for Mobile PhoneCAS: 103598-77-2Information provided by LG Chemical |
|||
Front Barrel Temperature | 275 - 280 °C | 527 - 536 °F | |
Lavergne VYPET VNT 230 PET - PBT 30% Glass Reinforced Polyester Vypet VNT 230 is a 30% fiberglass reinforced modified PBT/PET polyester injection molding compound designed for electrical applications requiring improved surface aesthetics and improved UV resistan.. |
|||
Front Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Start Point: 240°C |
Kingfa MAC-601 AC PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic partsComputer and accessoriesHou.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Start Point: 265°C |
Kingfa PA6-G30 N101 30% Glass Fiber Reinforced PA6 (general purpose) Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Start Point: 265°C |
Kingfa PA6-M20G16 20% Glass & 16% Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Start Point: 265°C |
Kingfa PA6-T25 25% Mineral Filled PA6 Features:Low tendency to wrapApplications:Injection moldingSport applianceAutomobile partsPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Front Barrel Temperature | 270 - 280 °C | 518 - 536 °F | |
Solvay TECHNYL® B 216 Natural D PA66/6, DRY Description: Unreinforced copolyamide 66/6, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 216 offers an excellent combination between impact resistance,.. |
|||
Front Barrel Temperature | 270 - 280 °C | 518 - 536 °F | |
Solvay TECHNYL® B 216 V30 Black 3 N PA66, 30% glass fiber, DRY Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 216 V30 is used in all sectors of in.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | |
Solvay TECHNYL® C 236SI PA6, DRY Description: Unreinforced polyamide 6 with high impact strength for injection molding.Available in: Europe and North AmericaProduct Applications: TECHNYL® C 236SI has high impact strength and fle.. |
|||
Front Barrel Temperature | 270 - 280 °C | 518 - 536 °F | |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Dry) Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur.. |
|||
Front Barrel Temperature | 240 - 280 °C | 464 - 536 °F | Injection Molding |
Styrolution Luran® S 777 K ASA Luran S 777 K is an easy flowing injection molding ASA grade with good toughness and heat distorsion resistance. |
|||
Front Barrel Temperature | 230 - 280 °C | 446 - 536 °F | |
Teknor Apex Beetle® MDF50 Nylon 6, 50% Short Glass Fiber Filler Notes: MDF50 is a 50% glass fiber reinforced nylon 6 that offers excellent mechanical performance coupled with good surface finish Features: Good Surface FinishProcessing Method: Injection molding F.. |
|||
Front Barrel Temperature | 250 - 280 °C | 482 - 536 °F | |
Teknor Apex Beetle® PBTC115F Polybutylene Terephthalate and Polyethylene Terephthalate Notes: PBTC115F is a 15% glass fiber reinforced PBT/PET alloy. It provides a good balance of mechanical performance and thermal endurance with excellent surface finish and mold release. Features: G.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Pre-3. Region Temperature |
Tisan TISLAMID® 66 15% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Pre-3. Region Temperature |
Tisan TISLAMID® 66 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Pre-3. Region Temperature |
Tisan TISLAMID® 66 20% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Pre-3. Region Temperature |
Tisan TISLAMID® 66 30% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Pre-3. Region Temperature |
Tisan TISLAMID® 66 Flame Retardant (V0). Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Pre-3. Region Temperature |
Tisan TISLAMID® 66 Impact Modified Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Pre-3. Region Temperature |
Tisan TISLAMID® 66 UNR Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Front Barrel Temperature | 270 - 280 °C | 518 - 536 °F | |
Celanese VECTRAN™ V100P Co-Extrudable Liquid Crystal Polymer (LCP) Description: PRELIMINARY DATA SHEET: Co-extrudable LCP for Barrier Applications. Vectran V100P Liquid Crystal Polymer is characterized by its excellent barrier properties independent of relative hum.. |
|||
Front Barrel Temperature | 275 - 280 °C | 527 - 536 °F | |
Celanese Impet® 340R PET, 45% Glass Reinforced
(Unverified Data**) Impet 340R is a 45% glass-reinforced injection moldable polyester made with post consumer recycled PET. It provides an excellent combination of strength, stiffness, and high temperature resistance.4.. |