Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Front Barrel Temperature = 536 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 275 - 280 °C
527 - 536 °F
Celanese Impet® 330R PET, 30% Glass Reinforced  (Unverified Data**)
Impet 330R is a 30% glass reinforced injection moldable polyester containing post consumer recycled PET. It provides an excellent combination of strength, stiffness, and high temperature resistance...
Front Barrel Temperature 270 - 280 °C
518 - 536 °F
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Natural..
Front Barrel Temperature 250 - 280 °C
482 - 536 °F
Start Point: 255°C
Kingfa JH710 G10D Flame Retardant & 10% Glass Fiber Reinforced PC
Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:Exact mechanism partsElectrical and elect..
Front Barrel Temperature 250 - 280 °C
482 - 536 °F
Start Point: 240°C
Kingfa MAC-601 UV PC/ABS Alloy
Features:Excellent balance propertiesHigh impact strengthGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic partsComputer and accessoriesHou..
Front Barrel Temperature 260 - 280 °C
500 - 536 °F
Start Point: 265°C
Kingfa PA6-G50 50% Glass Fiber Reinforced PA6
Features:Good size stabilityLow tendency to wrapHigh mechanical propertiesGood low temperature resistanceGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower t..
Front Barrel Temperature 250 - 280 °C
482 - 536 °F
Injection Molding
LG Chemical LUMID HI1202A(W) PA6, High Impact
Feature: Injection Molding, PA6, High ImpactApplication: Electric/Electronic PartsCAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical
Front Barrel Temperature 250 - 280 °C
482 - 536 °F
Injection Molding
LG Chemical LUPOY HP5004A PC/ABS
Description: Injection Molding, PC/ABS, General Purpose, Good Weld Properties, High Impact (at Low Temperature), Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2, 9003-56-9 and 18102..
Front Barrel Temperature 240 - 280 °C
464 - 536 °F
LG Chemical LUPOY HR-5007AX Heat Resistant PC/ABS Alloy, Unreinforced
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Front Barrel Temperature 265 - 280 °C
509 - 536 °F
Injection Molding
LG Chemical LUPOY SC5004T PC/Polyester, Transparency
Description: Injection Molding, PC/Polyester, General Purpose, Transparency, High FlowApplication: Keypad for Mobile PhoneCAS: 103598-77-2Information provided by LG Chemical
Front Barrel Temperature 250 - 280 °C
482 - 536 °F
Start Point: 255°C
Kingfa JH710 G20 Flame Retardant & 20% Glass Fiber Reinforced PC
Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc..
Front Barrel Temperature 250 - 280 °C
482 - 536 °F
Start Point: 240°C
Kingfa MAC-601 AC PC/ABS Alloy
Features:Excellent balance propertiesHigh impact strengthGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic partsComputer and accessoriesHou..
Front Barrel Temperature 275 - 280 °C
527 - 536 °F
Lavergne VYPET VNT 215 PET - PBT 15% Glass Reinforced Polyester
Vypet VNT 215 is a 15% fiberglass reinforced PET/PBT injection molding compound designed for structural applications.Features: High temperature performance; Low warp; High quality surfaceTypical App..
Front Barrel Temperature 275 - 280 °C
527 - 536 °F
Solvay TECHNYL® A 230 PA66, DRY
Description: Unreinforced and modified polyamide 66, with improved impact resistance, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHNYL® A 230 offers excel..
Front Barrel Temperature 270 - 280 °C
518 - 536 °F
Solvay TECHNYL® B 216 Natural D PA66/6, DRY
Description: Unreinforced copolyamide 66/6, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 216 offers an excellent combination between impact resistance,..
Front Barrel Temperature 270 - 280 °C
518 - 536 °F
Solvay TECHNYL® B 216 V30 Black 3 N PA66, 30% glass fiber, DRY
Description: Copolyamide 66/6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 216 V30 is used in all sectors of in..
Front Barrel Temperature 240 - 280 °C
464 - 536 °F
Solvay TECHNYL® C 538XT V30 Natural W PA6, 30% glass filled, DRY
Description: Polyamide 6 reinforced with 30% of glass fibers, heat stabilized, with high viscosity and high toughness, for extrusion.Available in: North America Product Applications: This product is..
Front Barrel Temperature 240 - 280 °C
464 - 536 °F
Teknor Apex Beetle® MDF2 Nylon 6, 30% Short Glass Fiber Reinforced, Dry
Notes: MDF2 is a heat stabilized 30% glass fiber reinforced nylon 6 that offers good mechanical performance coupled with good surface finish. Features: Heat Stabilized; Good Surface Finish Processin..
Front Barrel Temperature 250 - 280 °C
482 - 536 °F
Teknor Apex Beetle® PBTC115F Polybutylene Terephthalate and Polyethylene Terephthalate
Notes: PBTC115F is a 15% glass fiber reinforced PBT/PET alloy. It provides a good balance of mechanical performance and thermal endurance with excellent surface finish and mold release. Features: G..
Front Barrel Temperature 260 - 280 °C
500 - 536 °F
Teknor Apex Beetle® PET166F Polyethylene Terephthalate, 30% Glass Fiber Reinforced
Notes: PET166F is a 30% glass fiber reinforced grade of PET that offers good mechanical performance at elevated temperature and excellent mold release. Processing Method: Injection Molding Forms: Pe..
Front Barrel Temperature 260 - 280 °C
500 - 536 °F
Pre-3. Region Temperature
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Front Barrel Temperature 260 - 280 °C
500 - 536 °F
Pre-3. Region Temperature
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Front Barrel Temperature 260 - 280 °C
500 - 536 °F
Pre-3. Region Temperature
Tisan TISLAMID® 66 30% Glass Fiber Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Front Barrel Temperature 260 - 280 °C
500 - 536 °F
Pre-3. Region Temperature
Tisan TISLAMID® 66 30% Mineral Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Front Barrel Temperature 260 - 280 °C
500 - 536 °F
Pre-3. Region Temperature
Tisan TISLAMID® 66 Flame Retardant (V0). Heat Stabilized Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Front Barrel Temperature 260 - 280 °C
500 - 536 °F
Pre-3. Region Temperature
Tisan TISLAMID® 66 UNR Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Front Barrel Temperature 270 - 280 °C
518 - 536 °F
Zone 3
Eurostar Starflam RF0057P PA66/6, 25% Glass Filled, Injection Molded
Starflam RF0057P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym..
Front Barrel Temperature 265 - 280 °C
509 - 536 °F
Zone 3
Eurostar Starflam RF0077P PA66/6, 35% Glass Filled, Injection Molded
Starflam RF0077P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1007Z270EM)Information provided by Polym..
Front Barrel Temperature 270 - 280 °C
518 - 536 °F
Zone 3
Eurostar Starflam RF0097P PA66/6, 45% Glass Filled, Injection Molded
Starflam RF0097P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1009Z270EM)Information provided by Polym..
Front Barrel Temperature 275 - 280 °C
527 - 536 °F
Celanese Impet® 340R PET, 45% Glass Reinforced  (Unverified Data**)
Impet 340R is a 45% glass-reinforced injection moldable polyester made with post consumer recycled PET. It provides an excellent combination of strength, stiffness, and high temperature resistance.4..
Front Barrel Temperature 275 - 280 °C
527 - 536 °F
Celanese Impet® 830R PET, 35% Mineral / Glass Reinforced  (Unverified Data**)
Impet 830R is a 35% glass/mineral reinforced injection moldable polyester made with recycled PET. It provides an excellent combination of strength, stiffness, warp resistance, and high temperature c..