Polymer Property : Nozzle Temperature = 240 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Nozzle Temperature 240 - 260 °C
464 - 500 °F
PolyOne Bergamid™ XP6042701 Polyamide 6 (Nylon 6)
Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3.5 sec Cycle Time: 18 to 60 secInformation provided by PolyOne
Nozzle Temperature 240 - 270 °C
464 - 518 °F
Average value: 255 °C Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..
Nozzle Temperature 240 - 250 °C
464 - 482 °F
Samyang Triloy® 410 PC/PET alloy  (discontinued **)
Characteristics:Impact resistantHeat resistantDimensional stabilityProcessabilityGood flowApplications:O/A partRear view mirror housingRice cooker baseAll information provided by Samyang
Nozzle Temperature 240 - 250 °C
464 - 482 °F
Samyang Triloy® 410N PC/PET alloy, Flame Retardant  (discontinued **)
Characteristics:Impact resistantHeat resistantDimensional stabilityProcessabilityFlame retardantApplications:O/A partRear view mirror housingRice cooker baseAll information provided by Samyang
Nozzle Temperature 240 - 270 °C
464 - 518 °F
Nilit Nilamid B3 H ZA Unfilled, Low Temperature Impact Resistant PA6
Description: Nilamid B3 H ZA is a NYLON 6 with a low level of impact modification, allowing parts to be snap fitted in a dry-as-molded condition. It also has improved impact strength and elongation,..
Nozzle Temperature 240 - 310 °C
464 - 590 °F
Average value: 279 °C Grade Count:7
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
Nozzle Temperature 240 - 295 °C
464 - 563 °F
Average value: 269 °C Grade Count:8
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..
Nozzle Temperature 240 - 295 °C
464 - 563 °F
Akro-Plastic Akromid® S3 GF 30 4 (3552) PA 6.10 Dry, 30% Glass Filled  (discontinued **)
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Nozzle Temperature 240 - 270 °C
464 - 518 °F
Injection Molding
LG Chemical LUMID GP2251AF PA6+GF25%, Flame Retardant
Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical
Nozzle Temperature 240 - 250 °C
464 - 482 °F
Injection Molding
LG Chemical Lupox® GP1000S PBT
Description: Injection Molding, PBT, General PurposeApplication: Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical
Nozzle Temperature 240 - 260 °C
464 - 500 °F
LG Chemical Lupox® PBT-GP-2150 15% GFR PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Nozzle Temperature 240 - 260 °C
464 - 500 °F
LG Chemical Lupox® PBT-GP-2156F 15% GFR Flame Retardant PBT
General Purpose PBT, 15% Glass Fiber Reinforced, Weather Resistant, Flame Retardant, Non-Bleed. Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Nozzle Temperature 240 - 250 °C
464 - 482 °F
Injection Molding
LG Chemical XR474 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior HousingCAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical
Nozzle Temperature 240 - 250 °C
464 - 482 °F
Samyang Triloy® 120H PC/ABS alloy
Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityGood flowApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang
Nozzle Temperature 240 - 250 °C
464 - 482 °F
Samyang Triloy® 170 PC/PBT alloy
Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityFlame retardantApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang
Nozzle Temperature 240 - 250 °C
464 - 482 °F
Samyang Triloy® 210 PC/ABS alloy
Characteristics:Impact resistantHeat resistantGood flowApplications:Camera partsExterior panelCluster fasciaWheel coverStructural applicationI/P. core panelHelmet shellGlove box doorCowl vent grillA..
Nozzle Temperature 240 - 300 °C
464 - 572 °F
Topas Advanced Polymers TOPAS® 6013S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 6013S-04 is a general purpose injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance,..
Nozzle Temperature 240 °C
464 °F
Zhejiang Juner 301-G20 20% Glass Fibre Reinforced and Flammable Resistant
Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, ..
Nozzle Temperature 240 °C
464 °F
Recommended
Arkema Group Pebax® 5533 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 5533 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide..
Nozzle Temperature 240 °C
464 °F
Recommended
Arkema Group Pebax® Rnew 40R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 40R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..
Nozzle Temperature 240 - 280 °C
464 - 536 °F
Akro-Plastic Akromid® B3 GF 50 RM-M (3146) PA 6 Dry, 50% Glass Filled
In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele..
Nozzle Temperature 240 - 270 °C
464 - 518 °F
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM
Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri..
Nozzle Temperature 240 °C
464 °F
Beijing Ranger Chem PBT 403 M-G0 HF Halogen Free Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Nozzle Temperature 240 °C
464 °F
Beijing Ranger Chem PBT 403 M-G10 HF Halogen Free Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Nozzle Temperature 240 °C
464 °F
Beijing Ranger Chem PBT-MFC-G20 FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Nozzle Temperature 240 - 280 °C
464 - 536 °F
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Dry, 10% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Nozzle Temperature 240 - 280 °C
464 - 536 °F
Akro-Plastic Akromid® B3 GF 25 (2471) PA 6 Dry, 25% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Nozzle Temperature 240 - 295 °C
464 - 563 °F
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Nozzle Temperature 240 - 295 °C
464 - 563 °F
Akro-Plastic Akromid® S3 GF15 1 (3223) PA 6.10 Dry, 15% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..