Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 120 °C | 248 °F | |
Nanocyl PLASTICYL™ PC1501 Polycarbonate with 2 wt% Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Solvay Specialty Polymers Ixef® 1025 Polyarylamide (PARA)
(Unverified Data**) Ixef 1025 is a 50% glass-fiber reinforced, UV stabilized polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 1025/9.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA)
(Unverified Data**) Ixef 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance. - Natural: Ixef 1521/0.. |
|||
Mold Temperature | 120 - 130 °C | 248 - 266 °F | |
LATI LASULF Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Lehmann & Voss LUVOCOM® 19-7276 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Lehmann & Voss LUVOCOM® 19-7416 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Lehmann & Voss LUVOCOM® 19-7816 Polyamide 46, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Lehmann & Voss LUVOCOM® 19-7912 Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.Gear parts f.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Lehmann & Voss LUVOCOM® 19-8094 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Lehmann & Voss LUVOCOM® 19-8195/FR Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Lehmann & Voss LUVOCOM® 19-8365 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
LATI Lasulf G/20 PSU, 20% Glass Fiber Reinforced Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort.. |
|||
Mold Temperature | 120 - 200 °C | 248 - 392 °F | |
Lehmann & Voss LUVOCOM® 1100-8301 Polyether sulfone, with carbon fiber, PTFE, lubricant modified Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Strong, stiff parts.Dy.. |
|||
Mold Temperature | 120 - 200 °C | 248 - 392 °F | |
Lehmann & Voss LUVOCOM® 1100-8325 Polyether sulfone, with glass fiber and PTFE Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Improved friction and .. |
|||
Mold Temperature | 120 - 200 °C | 248 - 392 °F | |
Lehmann & Voss LUVOCOM® 1100/GF/20/EM/MR/BK Polyether sulfone, with glass fiber, easy flowing, demolding aid Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Mold Temperature | 120 - 200 °C | 248 - 392 °F | |
Lehmann & Voss LUVOCOM® 1100-8134 Polyether sulfone, with carbon fiber Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Solvay Specialty Polymers Ixef® 1622 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® 1622 is an impact modified, 50% glass-fiber reinforced polyarylamide. which exhibits very high strength and rigidity, outstanding surface gloss, and excellent impact resistance.Features: Go.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Solvay Specialty Polymers Ixef® 1622 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1622 is an impact modified, 50% glass-fiber reinforced polyarylamide. which exhibits very high strength and rigidity, outstanding surface gloss, and excellent impact resistance.Features: Go.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Solvay Specialty Polymers Ixef® FC-1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® FC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Teknor Apex Beetle® PET1610F Polyethylene Terephthalate, 50% Glass Fiber Reinforced Notes: PET1610F is a 50% glass fiber reinforced grade of PET that offers good mechanical performance at elevated temperatures and excellent mold release. Processing Method: Injection Molding Forms: .. |
|||
Mold Temperature | 120 °C | 248 °F | |
Toyobo ECOVYLOPET® EMC2301E PET Bottle Recycling Grade, 15% Filler Reinforced Features: PET Bottle Recycling Grade, 15% Filler Reinforced, Modified TypeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | actual surface temp |
Unitika P-1001A Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | actual surface temp |
Unitika UG-100-30 Engineering Plastic Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Covestro Apec® 1897 Polycarbonate Easy flowingeasy to demoldUV-stabilizedsoftening temperature (VST/B 120)=182 °CPreprocessingMax. Water content |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Eurotec® Tecopet® PT74 GR20 BK002 XA20 PET, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, black Information provided by Eurotec® |
|||
Mold Temperature | 120 - 160 °C | 248 - 320 °F | Injection molding |
BASF Ultrason® S 3010 MR UN PSU Description: Unreinforced, higher viscosity injection molding and extrusion grade, tougher, with improved chemical resistance and demolding optimized. Abbreviated designation according to ISO 1043-1.. |
|||
Mold Temperature | 120 - 200 °C | 248 - 392 °F | Average value: 157 °C Grade Count:28 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | Needed to develop high crystallinity |
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, DAM
(discontinued **)&l Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | Needed to develop high crystallinity |
Solvay Specialty Polymers Ixef® 2010/X914 Polyarylamide, 40% Filler, at Equilibrium (65% RH)
(discontinued ** The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Mold Temperature | 120 - 140 °C | 248 - 284 °F | |
Solvay Specialty Polymers Ixef® 5002 Polyarylamide (PARA), 20% GlassPTFE
(discontinued **) Ixef 5002 is a 20% glass-fiber reinforced, PTFE modified polyarylamide which exhibits very good mechanical performance, very good surface gloss, and superior wear properties.- Natural: Ixef 5002/008.. |