Processing Properties Metric English Comments
Mold Temperature 120 - 140 °C
248 - 284 °F
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance. - Natural: Ixef 1521/0..
Mold Temperature 120 - 140 °C
248 - 284 °F
Solvay Specialty Polymers Ixef® GS-1022 Polyarylamide (PARA)  (Unverified Data**)
Ixef GS-1022 is a 50% glass-fiber reinforced grade of polyarylamide (PARA) available in several colors. Parts molded from these colored resins can withstand high-energy gamma radiation without signi..
Mold Temperature 120 - 140 °C
248 - 284 °F
Needed to develop high crystallinity
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, at Equilibrium (65% RH)  (discontin
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
Mold Temperature 120 - 130 °C
248 - 266 °F
LATI LASULF Polysulfone (PSU)  (Unverified Data**)
Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi..
Mold Temperature 120 - 140 °C
248 - 284 °F
Solvay Specialty Polymers Ixef® 2057 Polyarylamide (PARA), 45% Mineral Filler  (discontinued **)
Ixef 2057 is a 45% mineral-reinforced polyarylamide which exhibits high strength and stiffness, and outstanding surface gloss. Due to its mineral reinforcement, Ixef 2057 resin mold with very low wa..
Mold Temperature 120 - 140 °C
248 - 284 °F
Solvay Specialty Polymers Ixef® 2011 Polyarylamide (PARA), 42% Mineral Filler  (discontinued **)
Ixef 2011 is a general purpose, 42% mineral reinforcedpolyarylamide which exhibits high strength and stiffness, low warpage, and outstanding surface gloss.- Black: Ixef 2011/9000- Custom ColorableFe..
Mold Temperature 120 - 140 °C
248 - 284 °F
Lehmann & Voss LUVOCOM® 19-7312/GN Polyamide 46, with glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot..
Mold Temperature 120 - 140 °C
248 - 284 °F
Lehmann & Voss LUVOCOM® 19-7416 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Mold Temperature 120 - 140 °C
248 - 284 °F
Lehmann & Voss LUVOCOM® 19-7748 Polyamide 46, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Mold Temperature 120 - 140 °C
248 - 284 °F
Lehmann & Voss LUVOCOM® 19-7900 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Mold Temperature 120 - 140 °C
248 - 284 °F
Lehmann & Voss LUVOCOM® 19-8073 Polyamide 46, with aramid reinforcement and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert..
Mold Temperature 120 - 150 °C
248 - 302 °F
Injection Molding
LG Chemical LUSEP GP2400 PPS+GF40%, General Purpose
Feature: Injection Molding, PPS+GF40%, General PurposeApplication: Pump Units, Motor Units, etc.CAS No. 25212-74-2 and 65997-17-3Information provided by LG Chemical
Mold Temperature 120 - 140 °C
248 - 284 °F
LATI Lasulf G/15 PSU, 15% Glass Fiber Reinforced
Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort..
Mold Temperature 120 - 140 °C
248 - 284 °F
Lehmann & Voss LUVOCOM® 19-7745 Polyamide 46, with PTFE, improved wear resistance
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Good friction and wear behaviour especially at increased te..
Mold Temperature 120 - 140 °C
248 - 284 °F
LATI Lasulf G/30 PSU, 30% Glass Fiber Reinforced
Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort..
Mold Temperature 120 - 200 °C
248 - 392 °F
Lehmann & Voss LUVOCOM® 1100-7721/WT9016 Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Mold Temperature 120 - 200 °C
248 - 392 °F
Lehmann & Voss LUVOCOM® 1100-8166 Polyether sulfone, with glass fiber, easy flowing
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Mold Temperature 120 - 140 °C
248 - 284 °F
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feature..
Mold Temperature 120 - 140 °C
248 - 284 °F
Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA), 30% Carbon Fiber
Ixef® 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than gla..
Mold Temperature 120 - 160 °C
248 - 320 °F
Solvay Specialty Polymers Veradel® 3320GF Polyethersulfone (PESU), 20% Glass Fiber
Veradel® 3320GF is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, ..
Mold Temperature 120 - 140 °C
248 - 284 °F
Teknor Apex Beetle® PET166F Polyethylene Terephthalate, 30% Glass Fiber Reinforced
Notes: PET166F is a 30% glass fiber reinforced grade of PET that offers good mechanical performance at elevated temperature and excellent mold release. Processing Method: Injection Molding Forms: Pe..
Mold Temperature 120 - 140 °C
248 - 284 °F
actual surface temp
Unitika L-1003PA
Heat resistance, creep resistance, and excellent lubricantInformation provided by Unitika Ltd.
Mold Temperature 120 °C
248 °F
Toyobo ECOVYLOPET® EMC2311 PET Bottle Recycling Grade, 10% Glass Reinforced
Features: PET Bottle Recycling Grade, 10% Glass Fiber Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo..
Mold Temperature 120 - 140 °C
248 - 284 °F
Toyobo GLAMIDE® T-663G50A MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Mold Temperature 120 - 140 °C
248 - 284 °F
Eurotec® Tecopet® PT74 GR20 BK002 XA20 PET, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, black
Information provided by Eurotec®
Mold Temperature 120 - 200 °C
248 - 392 °F
Average value: 158 °C Grade Count:17
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a..
Mold Temperature 120 - 200 °C
248 - 392 °F
Average value: 157 °C Grade Count:28
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu..
Mold Temperature 120 - 160 °C
248 - 320 °F
Solvay Specialty Polymers Veradel® 3320GF Polyethersulfone (PESU)  (Unverified Data**)
Veradel 3320GF is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime..
Mold Temperature 120 - 140 °C
248 - 284 °F
Needed to develop high crystallinity
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, DAM  (discontinued **)&l
Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu..
Mold Temperature 120 - 140 °C
248 - 284 °F
Needed to develop high crystallinity
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, DAM  (discontinued **)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..