Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Mold Temperature = 239 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 115 - 130 °C
239 - 266 °F
Solvay Specialty Polymers Kalix® 5950 HFFR Polyamide, High Performance (HPPA), 50% Glass Fiber
Kalix® 5950 HFFR is a halogen-free, flame retardant (UL-94 V0 at 0.4 mm), highly reinforced polyamide material specifically formulated for high strength and stiffness applications where good impa..
Mold Temperature 115 °C
239 °F
Injection molding
BASF Petra® 110 BK-112 15% Glass Filled PET
Petra 110 is a 15% glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a good combination of performance properties including good strength a..
Mold Temperature 115 °C
239 °F
Injection molding
BASF Petra® 130 30% Glass Filled PET
Petra 130 is a 30% glass fiber reinforced polyethylene terephthalate (PET) for injection molding applications. It exhibits a good combination of performance properties including high strength and s..
Mold Temperature 115 °C
239 °F
Injection molding
BASF Petra® 130 BK-112 30% Glass Filled PET
Petra 130 BK-112 is a 30% glass fiber reinforced, black pigmented polyethylene terephthalate injection molding compound. It exhibits a combination of performance properties including good strength ..
Mold Temperature 115 °C
239 °F
Injection molding
BASF Petra® 130 FR 30% Glass Filled PET
Petra 130 FR is a 30% glass fiber reinforced, flame retardant injection molding polyethylene terephthalate feedstocks. It is recognized as UL 94V-0/5VA by Underwriters Laboratories. It is also avail..
Mold Temperature 115 °C
239 °F
Injection molding
BASF Petra® 130 FR BK-112 30% Glass Filled PET
Petra 130 FR BK-112 is a 30% glass fiber reinforced, black pigmented, flame retardant injection molding compound based on post-consumer and post-industrial recycle polyethylene erephthalate feedstoc..
Mold Temperature 115 °C
239 °F
Injection molding
BASF Petra® 140 45% Glass Filled PET
Petra 140 is a 45% glass reinforced injection molding polyethylene terephthalate (PET) offering an increased level of strength, stiffness, high temperature performance and dimensional stability. Ex..
Mold Temperature 115 °C
239 °F
Injection molding
BASF Petra® 140 BK-112 45% Glass Filled PET
Petra 140 BK-112 is a 45% glass reinforced, pigmented black, polyethylene terephthalate (PET) injection molding compound offering an increased level of strength, stiffness, high temperature performa..
Mold Temperature 115 °C
239 °F
Injection molding
BASF Petra® 7030 GY6128 30% Glass Filled PET
Petra 7030 GY6128 is a grey pigmented, high flow 30% glass fiber reinforced injection molding compound based on post-consumer and post-industrial recycled polyethylene terephthalate feedstock. It o..
Mold Temperature 115 °C
239 °F
Injection molding
BASF Petra® 230 BK-112 22/13% Glass/Mineral Filled PET
Petra 230 BK-112 is a 35% mineral and glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a very good combination of performance properties in..