Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Trilliant™ HC HC6200-5002 XR Grey Polyamide 12 (Nylon 12)

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer PolyOne Corporation
Trade Name Trilliant™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Trilliant™ HC HC6200-5002 XR Grey Polyamide 12 (Nylon 12).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead of competition. When specified, Trilliant® compound may incorporate agency rated materials that meet USP Class IV, FDA or ISO 10993 testing requirements. This Trilliant® grade is a high density specialty compound featuring a sustainable material solution for radiation shielding and weighting & balancing applications. The composite material offers a high performance thermoplastic-based alternative to lead. This compound has densities similar to traditional metals and provides greater flexibility in design and processing.Shielding properties: Attenuation coefficient at 511 keV = 0.72cm-1 Half Thickness at 511 keV = 0.96cmInformation provided by PolyOne
Physical Properties Metric English Comments
Density 8.00 g/cc
0.289 lb/in³
ISO 1183
Linear Mold Shrinkage 0.010 - 0.015 cm/cm
0.010 - 0.015 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
ISO 527-2/50
Elongation at Break 1.0 - 2.0 %
1.0 - 2.0 %
ISO 527-2/50
Tensile Modulus 5.00 GPa
725 ksi
ISO 527-2/1
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Thermal Conductivity 1.50 - 2.00 W/m-K
10.4 - 13.9 BTU-in/hr-ft²-°F
ASTM E1461
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
Unannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
Unannealed; ISO 75-2/A
Electrical Properties Metric English Comments
Surface Resistance <= 1000 ohm
<= 1000 ohm
IEC 60093
Processing Properties Metric English Comments
Melt Temperature 230 - 280 °C
446 - 536 °F
Mold Temperature 65.0 - 100 °C
149 - 212 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4.00 hour
4.00 hour
Descriptive Properties Value Comments
Appearance Grey
Features High Specific Gravity
Medium Impact Resistance
Non-Toxic
Forms Pellets
Generic Material Nylon 12
Generic Name Polyamide 12 (Nylon 12)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Housings
Medical/Healthcare Applications
Radiation Shielding
Weighting & Balancing
Users viewing this material also viewed the following: