Processing Properties Metric English Comments
Drying Temperature 149 - 163 °C
300 - 325 °F
Average value: 149 °C Grade Count:13
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Carbon Fiber Filled". Each property range of values reported is minimum an..
Drying Temperature 149 - 163 °C
300 - 325 °F
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU)  (Unverified Data**)
Udel GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resista..
Drying Temperature 149 - 163 °C
300 - 325 °F
Solvay Specialty Polymers Udel® GF-120 Polysulfone (PSU)  (Unverified Data**)
Udel GF-120, resin is a 20% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resi..
Drying Temperature 135 - 163 °C
275 - 325 °F
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU)  (Unverified Data**)
Udel P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand prolonged e..
Drying Temperature 135 - 163 °C
275 - 325 °F
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU)  (Unverified Data**)
Udel P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and withsta..
Drying Temperature 135 - 163 °C
275 - 325 °F
Solvay Specialty Polymers Udel® P-1720 Polysulfone (PSU)  (discontinued **)
Udel P-1720 is a flame-retardant grade of polysulfone (PSU) that has a UL94 rating of V-0 at a thickness of 1 mm (0.039"). In general, polysulfone is a tough, rigid, high-strength thermoplastic that..
Drying Temperature 135 - 163 °C
275 - 325 °F
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU)  (Unverified Data**)
Udel P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded. Polysulfones have long been known for trans..
Drying Temperature 135 - 163 °C
275 - 325 °F
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU)  (Unverified Data**)
Udel P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion. Th..
Drying Temperature 135 - 163 °C
275 - 325 °F
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU)  (Unverified Data**)
Udel polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel P-3500 LCD MB series polymers are particularly well suited for the fabrication of porous ..
Drying Temperature 135 - 163 °C
275 - 325 °F
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU)  (Unverified Data**)
Udel P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel P-1700 and a slightly greater t..
Drying Temperature 135 - 163 °C

@Time 10800 - 14400 sec
275 - 325 °F

@Time 3.00 - 4.00 hour
Solvay Specialty Polymers Mindel® B-322 Polysulfone, Modified (PSU, Modified)  (discontinued **)
Mindel B-322 is a glass filled, modified polysulfone developed specifically for molded electrical connector applications requiring excellent dimensional stability and resistance to warpage. This mat..
Drying Temperature 135 - 163 °C

@Time 10800 - 14400 sec
275 - 325 °F

@Time 3.00 - 4.00 hour
Solvay Specialty Polymers Mindel® B-430 Polysulfone, Modified (PSU, Modified)  (discontinued **)
Mindel B-430 is a 30% glass reinforced thermoplastic with excellent dimensional stability, exceptional resistance to warp, good chemical resistance, and high stiffness. It was developed specifically..
Drying Temperature 135 - 163 °C
275 - 325 °F
Solvay Specialty Polymers Udel® P-1800 Polysulfone (PSU)  (discontinued **)
Udel P-1800 is a powdered grade of polysulfone with molecular weight similar to that of Udel P-1700 polysulfone. It is well suited for the fabrication of porous membranes that can be made into hollo..
Drying Temperature 149 - 163 °C
300 - 325 °F
PolyOne Edgetek® LCP-15GF/000 Liquid Crystal Polymer - 15% Fiber Glass  (discontinued **)
Data provided by PolyOne.
Drying Temperature 149 - 163 °C
300 - 325 °F
PolyOne Edgetek® LCP-30CF/000 Liquid Crystal Polymer - 30% Carbon Fiber  (discontinued **)
Data provided by PolyOne.
Drying Temperature 149 - 163 °C

@Time 10800 - 14400 sec
300 - 325 °F

@Time 3.00 - 4.00 hour
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU), Glass Fiber
Udel® GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical res..
Drying Temperature 149 - 163 °C

@Time 10800 - 14400 sec
300 - 325 °F

@Time 3.00 - 4.00 hour
Solvay Specialty Polymers Udel® GF-120 Polysulfone (PSU), Glass Fiber
Udel® GF-120, resin is a 20% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical ..
Drying Temperature 135 - 163 °C

@Time 12600 sec
275 - 325 °F

@Time 3.50 hour
Solvay Specialty Polymers Udel® P-1710 Polysulfone (PSU)
Udel® P-1710 polysulfone (PSU) is a tough, rigid, high-strength thermoplastic that is suitable for continuous use up to 300°F (149°C). The resin is resistant to oxidation and hydrolysis and..
Drying Temperature 135 - 163 °C

@Time 12600 sec
275 - 325 °F

@Time 3.50 hour
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU)
Udel® P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded.Polysulfones have long been known for tr..
Drying Temperature 135 - 163 °C

@Time 12600 sec
275 - 325 °F

@Time 3.50 hour
Solvay Specialty Polymers Udel® P-3500 LCD MB Polysulfone (PSU)
Udel® polysulfone is a tough, rigid, high-strength thermoplastic with outstanding hydrolytic resistance. Udel® P-3500 LCD MB series polymers are particularly well suited for the fabrication of..
Drying Temperature 135 - 163 °C

@Time 12600 sec
275 - 325 °F

@Time 3.50 hour
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU)
Udel® P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion..
Drying Temperature 135 - 163 °C

@Time 12600 sec
275 - 325 °F

@Time 3.50 hour
Solvay Specialty Polymers Udel® P-3703 Polysulfone (PSU)
Udel® P-3703 is a high-flow grade of polysulfone intended for injection molding applications with thin walls or long flow lengths. This grade has higher flow than Udel® P-1700 and a slightly g..
Drying Temperature 135 - 163 °C

@Time 12600 sec
275 - 325 °F

@Time 3.50 hour
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU)
Udel® P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand pro..
Copyright © lookpolymers.com All Rights Reserved