Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.000 - 0.689 MPa | 0.000 - 99.9 psi | |
PolyOne Versaflex™ 9570-1 Thermoplastic Elastomer (TPE) Versaflex™ 9570-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Back Pressure | 0.000 - 0.689 MPa | 0.000 - 99.9 psi | |
PolyOne Versaflex™ OM 6160-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 6160-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell.. |
|||
Back Pressure | 0.000 - 0.689 MPa | 0.000 - 99.9 psi | |
PolyOne Versalloy™ HC 9210-70N Thermoplastic Elastomer (TPE) Versalloy™ HC 9210-70N is a USP Class VI, TPV alloy targeted for injection molding healthcare applications such as disposable medical items and soft-touch overmolding for surgical grips. Product ex.. |
|||
Back Pressure | 0.000 - 0.689 MPa | 0.000 - 99.9 psi | |
PolyOne Versalloy™ HC 9220-90 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-90 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Back Pressure | 0.000 - 0.689 MPa | 0.000 - 99.9 psi | |
PolyOne Dynaflex™ G7640-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7640-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Back Pressure | 0.000 - 0.689 MPa | 0.000 - 99.9 psi | |
PolyOne Dynaflex™ G7940-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Back Pressure | 0.000 - 0.689 MPa | 0.000 - 99.9 psi | |
PolyOne Dynaflex™ G7940-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP VALOX® SMV5846 PBT + PET Alloy, 20% Carbon Fiber Reinforcement
(discontinued **) ESD ApplicationsFeatures: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is .. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP Stat-Kon® LC-1003 Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP Stat-Kon® LC-1003 EM Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Features: Good Moldability, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; howev.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP Thermocomp® LF-1006 Polyetheretherketone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP Thermocomp® JF-1004 EM M BK905 Polyethersulfone, Milled Glass Fiber
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP Lubricomp® ECL-4036 Polyetherimide, Carbon Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP Lubricomp® EFL-4544 Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP Lubricomp® EL-4030 Polyetherimide, PTFE Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP Thermocomp® EC-1006 Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP Thermocomp® EF-1002 EP BK8-114 Polyetherimide, Glass Fiber Reinforcement
(discontinued **) Features: Good ProcessabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP Thermocomp® EF-1004 BK8-115 Polyetherimide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP ULTEM® UC3000 Polyetherimide, 30% Carbon Fiber Reinforcement
(discontinued **) High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP ULTEM® UCF1205 Polyetherimide, 12% Carbon Fiber Reinforcement, 5% PTFE Lubricant
(discontinued **) Office equipment internal parts.Features: Lubricated, Good Wear ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labe.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU), Glass Fiber Udel® GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical res.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
Solvay Specialty Polymers Udel® GF-120 Polysulfone (PSU), Glass Fiber Udel® GF-120, resin is a 20% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical .. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
Solvay Specialty Polymers Veradel® AG-320 Polyethersulfone (PESU), 20% Glass Fiber Veradel® AG-320 is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
ExxonMobil Santoprene® 8281-75MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP ULTEM® SMU5831 Polyetherimide, 30% CarbonGlassMineral Reinforced
(discontinued **) ESD characteristics for ultra high-heat applications. Will be UC3010H.Features: High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Compa.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP ULTEM® SMU5832 Polyetherimide, 30% CarbonGlassMineral Reinforced
(discontinued **) ESD characteristics for ultra high-heat applications. Will be UC3010.Features: High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Compan.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
Solvay Specialty Polymers Veradel® AG-320 Polyethersulfone (PESU)
(Unverified Data**) Veradel AG-320 is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP Lubricomp® JFL-4036 Polyethersulfone, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP Thermocomp® JF-1006 E LE BK8-055 Polyethersulfone, Glass Fiber Reinforcement
(discontinued **) Features: High Viscosity, Low ExtractablesForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many L.. |
|||
Back Pressure | 0.345 - 0.689 MPa | 50.0 - 99.9 psi | |
LNP ULTEM® SMU5836 Polyetherimide, 30% Carbon Fiber Reinforcement
(discontinued **) High modulus with shielding/ conductive characteristics for high-heat applications.Features: Electrically Conductive, High Heat Resistance, High StrengthForms: PelletsProcessing Method: Injection Mo.. |