Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
Plastcom SLOVAMID® 6 T 30 FRC 4 TS PA6 flame retarded, heat stabilized PA 6 for injection molding, reinforced with 30% mineral filler, flame retarded with nonhalogen flame retardant, heat stabilized. Main features: flammability in accordance with UL 94 3 at 1,6 mm, glo.. |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
Polykemi AB POLYelast TPE HJ-75 UV Thermoplastic Elastomer, PP/Elastomer/Mineral, UV-Stabilized, Low CLTE Information provided by Polykemi AB |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
Polykemi AB POLYfill PP CPQ10015 FF Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
Polykemi AB POLYfill PP CPX10030 UV Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
Polykemi AB POLYfill PP CQX10030 R3 Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
Melt Temperature | 230 - 270 °C | 446 - 518 °F | |
PolyOne Bergadur™ PB400 G30 UF UV Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Melt Temperature | <= 230 °C | <= 446 °F | |
Panipol Oy DXH Inherently Conductive Polymer Panipol DXH composition is conductive masterbatch for melt processing with commodity polymers such as polypropylene. It is based on doped and plasticized Polyaniline. Benefits of Panipol DXH grade.. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | Average value: 257 °C Grade Count:19 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | Start Point: 230°C |
Kingfa JH960 6300 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platin.. |
|||
Melt Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
LG Chemical LUMAX GN5006FC PBT+ABS, Heat Resistance Description: Injection Molding, PBT+ABS, Halogen Free Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 9003-54-7 and 24968-12-5Information provided by LG Chemical |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical XR440 ABS, Low Emission High Heat ABS Feature: Injection Molding Grade, Low Emission High Heat ABSApplication: Automotives Interior housingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical |
|||
Melt Temperature | 230 - 280 °C | 446 - 536 °F | |
LATI Laticonther 52/11 GR/70 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Melt Temperature | 230 - 260 °C | 446 - 500 °F | |
Solvay Technyl® C216V15 15% Glass Filled Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Melt Temperature | 230 - 260 °C | 446 - 500 °F | |
Solvay Technyl® C216V30 30% Glass Filled Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Melt Temperature | 230 - 270 °C | 446 - 518 °F | ISO 294 |
Styrolution Novodur® 4000PG ABS Novodur Ultra 4000PG is an injection molding grade especially suitable for electroplating, providing enhanced heat resistance.Information provided by Styrolution |
|||
Melt Temperature | 230 - 270 °C | 446 - 518 °F | ISO 294 |
Styrolution Novodur® 4140PG ABS Novodur Ultra 4140PG is a PC modified plating grade combining high heat resistance and excellent impact strength with the unique surface properties of a Novodur ABS material.Information provided by .. |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
Lubrizol Isoplast® 2531 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-27 GF10 MX6 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grade, reinforced with 10% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good surface quality.T.. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-27 GF15 MW25 Polyamide 6 - Mineral Reinforced 15% Glass fiber reinforced and 25% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the followi.. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-27 MCS I8 Polyamide 6 - Impact Modified Increased impact resistance grade. Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main propert.. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-27 MX6 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grade, reinforced with 10% hybrid mineral-glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning, good su.. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-30 Polyamide 6 - Natural High viscosity extrusion grade for blown and flat films, including biaxial oriented films, also for extrusion of rods, pipes, plates, sheets, low diameter tubes and for injection molding of thick-wa.. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-27 M Polyamide 6 - Improved Slip Properties Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid.. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-27 MCS Polyamide 6 - Colored Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.For colored parts produced by injection molding.Tarnamid® has the following .. |
|||
Melt Temperature | 230 - 240 °C | 446 - 464 °F | |
Polyplastic Armlen® PP MF 40-2HS Polypropylene, 40% Mineral Filled Impact modified, injection moldingInformation provided by PolyPlastic Group. |
|||
Melt Temperature | 230 - 290 °C | 446 - 554 °F | |
Azoty Tarnow™ Tarnamid® T-27 GF25 M Polyamide 6 - Improved Slip Properties Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid.. |
|||
Melt Temperature | 230 - 250 °C | 446 - 482 °F | |
LATI Latiblend 6252 H2 G/30 PA6/PP Homopolymer Blend based on Polyamide 6 (PA6) / Polypropylene homopolymer (PPh). Heat stabilized. Glass fibers. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |