Processing Properties Metric English Comments
Melt Temperature 20.0 - 285 °C
68.0 - 545 °F
Average value: 236 °C Grade Count:18
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..
Melt Temperature 20.0 - 280 °C
68.0 - 536 °F
Average value: 254 °C Grade Count:12
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
Melt Temperature 20.0 - 371 °C
68.0 - 700 °F
Average value: 184 °C Grade Count:16
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
Melt Temperature 20.0 - 218 °C
68.0 - 425 °F
Average value: 173 °C Grade Count:13
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
Melt Temperature 20.0 - 215 °C
68.0 - 419 °F
Average value: 184 °C Grade Count:30
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m..
Melt Temperature 20.0 - 220 °C
68.0 - 428 °F
Average value: 203 °C Grade Count:10
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim..
Melt Temperature 20.0 - 399 °C
68.0 - 750 °F
Average value: 276 °C Grade Count:11
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an..
Melt Temperature 20.0 - 340 °C
68.0 - 644 °F
Average value: 292 °C Grade Count:12
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%..
Melt Temperature 20.0 - 345 °C
68.0 - 653 °F
Average value: 292 °C Grade Count:19
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%..
Melt Temperature 20.0 - 345 °C
68.0 - 653 °F
Average value: 286 °C Grade Count:11
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%..
Melt Temperature 20.0 - 277 °C
68.0 - 531 °F
Average value: 246 °C Grade Count:16
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..
Melt Temperature 20.0 - 300 °C
68.0 - 572 °F
Average value: 270 °C Grade Count:13
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..
Melt Temperature 20.0 - 300 °C
68.0 - 572 °F
Average value: 262 °C Grade Count:8
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..
Melt Temperature 20.0 - 304 °C
68.0 - 579 °F
Average value: 274 °C Grade Count:22
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m..
Melt Temperature 20.0 - 270 °C
68.0 - 518 °F
Average value: 231 °C Grade Count:15
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported..