Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Polymer Resources PC-BR1-UV Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilized Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilizedFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical.. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Polymer Resources PC-FR1-D Polycarbonate, Improved Flame Retardant, Low Flow Polycarbonate, Improved Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Polymer Resources PC-GP1-[color]-LF Polycarbonate, General Purpose, Food Contact Polycarbonate, General Purpose, Low FlowFeatures: • Food Contact AcceptableProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Polymer Resources PC-GP1-10TFE Polycarbonate, General Purpose, Wear Resistant, Low Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Polymer Resources PC-GP1-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Low Flow Polycarbonate, FDA-compliant Feedstocks, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro.. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Polymer Resources PC-GP1-TFE5 Polycarbonate, 5% PTFE, Wear Resistant, Low Flow Polycarbonate, 5% PTFE, General Purpose, Wear Resistant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Polymer Resources PC-HH Polycarbonate, High Heat Polycarbonate, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resource.. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Polymer Resources PC-UV1-D Polycarbonate, UV-stabilized, Low Flow Polycarbonate, UV-stabilized, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Po.. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
PTS Tristar® PC-10R-(V6) 6 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Polymer Resources PC-FD1 Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Polymer Resources PC-FR1-D-[color]-3 Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Polymer Resources PC-GP1-TFE10 Polycarbonate, 10% PTFE, Wear Resistant, Low Flow Polycarbonate, 10% PTFE, General Purpose, Wear Resistant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
PolyOne Stat-Tech™ LC-40CF/000 Natural LCP (Liquid Crystal Polymer), 40% Carbon Fiber Reinforced, Electrically Conductive, EMI/RFI Shielding Information provided by PolyOne™ Corporation |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | Molding |
PolyOne Edgetek® SF-20GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 316 - 332 °C | 600 - 630 °F | Molding |
PolyOne Lubri-Tech™ SF-30CF/13T2S Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced, PTFE/Silicone Lubricated
&n Description/Features:Carbon Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 316 - 327 °C | 600 - 620 °F | Molding |
PolyOne Edgetek® SF-30GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Mitsubishi Iupilon® E2000R 5 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Mitsubishi Iupilon® E2000UR 5 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Star Plastics PC733R Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Star Plastics PCGF10 Molding Grade PC with 10% Glass Information provided by Star Plastics, Inc. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Star Plastics PCGF20 Molding Grade PC with 20% Glass Information provided by Star Plastics, Inc. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Star Plastics PCGF30 Molding Grade PC with 30% Glass Information provided by Star Plastics, Inc. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | |
Samyang Trirex® PC-3027U 6 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Melt Temperature | 316 - 371 °C | 600 - 700 °F | Molding |
PolyOne Lubri-Tech™ PI-000/15T Polyetherimide (PEI), PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 316 °C | 600 °F | Molding |
PolyOne Edgetek® SF-45GF/000 Polyphenylene Sulfide (PPS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | Molding |
PolyOne Edgetek® AM-20CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | Molding |
PolyOne Edgetek® AM-30CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | Molding |
PolyOne Lubri-Tech™ AM-30CF/15T Polyphthalamide (PPA), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | Molding |
PolyOne Edgetek® AM-30GF/000 Polyphthalamide (PPA), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 316 - 343 °C | 600 - 650 °F | Molding |
PolyOne Edgetek® AM-30GM/15TF Polyphthalamide (PPA), Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |