Electrical Properties Metric English Comments
Surface Resistance 1.00 - 1.00e+14 ohm
1.00 - 1.00e+14 ohm
Average value: 1.28e+12 ohm Grade Count:43
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
Surface Resistance 1.00 - 1.00e+12 ohm
1.00 - 1.00e+12 ohm
Average value: 6.17e+10 ohm Grade Count:11
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Surface Resistance 1.00 - 1.00e+6 ohm
1.00 - 1.00e+6 ohm
Average value: 75200 ohm Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Surface Resistance 1.00 - 1.00e+6 ohm
1.00 - 1.00e+6 ohm
Average value: 252000 ohm Grade Count:27
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu..
Surface Resistance 1.00 - 1.00e+12 ohm
1.00 - 1.00e+12 ohm
Average value: 1.44e+10 ohm Grade Count:92
Overview of materials for Polycarbonate, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v..
Surface Resistance 1.00 - 1.00e+6 ohm
1.00 - 1.00e+6 ohm
Average value: 79600 ohm Grade Count:20
Overview of materials for Polycarbonate, NCG Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, NCG Filled". Each property range of values reported is minimum and maximum values of appr..
Surface Resistance 1.00 - 9.90e+11 ohm
1.00 - 9.90e+11 ohm
Average value: 2.42e+9 ohm Grade Count:25
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
Surface Resistance 1.00 - 1.00e+6 ohm
1.00 - 1.00e+6 ohm
Average value: 48800 ohm Grade Count:16
Overview of materials for Polyphenylene Sulfide (PPS), Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Conductive". Each property range of values reported is minimum and maximum ..
Surface Resistance 1.00 - 1.00e+16 ohm
1.00 - 1.00e+16 ohm
Average value: 8.14e+14 ohm Grade Count:69
Overview of materials for Nylon 66, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr..
Surface Resistance 1.00 - 1.00e+16 ohm
1.00 - 1.00e+16 ohm
Average value: 9.40e+14 ohm Grade Count:113
Overview of materials for Nylon 66, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr..
Surface Resistance 1.00 - 1.00e+13 ohm
1.00 - 1.00e+13 ohm
Average value: 2.00e+11 ohm Grade Count:40
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..
Surface Resistance 1.00 - 1.00e+10 ohm
1.00 - 1.00e+10 ohm
Average value: 4.17e+8 ohm Grade Count:28
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
Surface Resistance 1.00 - 1.00e+6 ohm
1.00 - 1.00e+6 ohm
Average value: 117000 ohm Grade Count:10
Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, NCG Fiber Filled". Each property range of values reported is minimum and maxim..
Surface Resistance 1.00 - 1.00e+6 ohm
1.00 - 1.00e+6 ohm
Average value: 319000 ohm Grade Count:18
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi..
Surface Resistance 1.00 - 5.20e+15 ohm
1.00 - 5.20e+15 ohm
Average value: 1.28e+14 ohm Grade Count:230
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
Surface Resistance 1.00 - 100 ohm
1.00 - 100 ohm
ASTM D257
Daelim H&L Plavis-C CM Conductive Polyimide Bearing
Compression Molded. Plavis-C: Conductive, Electrical conductive, high thermal resistance and superior mechanical properties. Surface resistivity 10²-10³ OhmGeneral Plavis information for all grad..
Surface Resistance 1.00 - 100 ohm
1.00 - 100 ohm
ASTM D257
Daelim H&L Plavis-C DF Conductive Polyimide Bearing
Direct Formed. Plavis-C: Conductive, Electrical conductive, high thermal resistance and superior mechanical properties. Surface resistivity 10²-10³ OhmGeneral Plavis information for all grades:PL..
Surface Resistance 1.00 - 1.00e+16 ohm
1.00 - 1.00e+16 ohm
Average value: 9.02e+14 ohm Grade Count:59
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
Surface Resistance 1.00 - 1.00e+6 ohm
1.00 - 1.00e+6 ohm
Average value: 573000 ohm Grade Count:7
Overview of materials for PC/ABS + Stainless Steel
This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro..
Surface Resistance 1.00 - 1.00e+7 ohm
1.00 - 1.00e+7 ohm
Average value: 363000 ohm Grade Count:43
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo..
Surface Resistance 1.00 - 9.90e+11 ohm
1.00 - 9.90e+11 ohm
Average value: 2.79e+10 ohm Grade Count:28
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max..
Surface Resistance 1.00 - 1.60e+17 ohm
1.00 - 1.60e+17 ohm
Average value: 5.70e+15 ohm Grade Count:271
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..
Copyright © lookpolymers.com All Rights Reserved