Electrical Properties Metric English Comments
Arc Resistance >= 130 sec
>= 130 sec
ASTM D495
Perstorp Compounds Aminel GF Melamine
Fiberglass-reinforced melamine material with high dimensional stability, excellent injection properties and high thermal stabilityInformation provided by Perstorp Compounds Inc.
Arc Resistance 130 sec
130 sec
ASTM D495
Celanese Celanex® 3100-2 PBT, 7.5% Glass Reinforced  (Unverified Data**)
Celanex 3100 is a general purpose, 7.5% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 3100 is a high flow material.7.5% glass-f..
Arc Resistance 130 - 180 sec
130 - 180 sec
Average value: 167 sec Grade Count:10
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values report..
Arc Resistance 130 sec
130 sec
Average value: 130 sec Grade Count:3
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma..
Arc Resistance 130 sec
130 sec
ASTM D495
Kolon KOLEFIN® KO133GM40 M/F Reinforced Polypropylene
KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica..
Arc Resistance 130 sec
130 sec
ASTM D495
Kolon KOLEFIN® KO133MT30 M/F Reinforced Polypropylene
KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica..
Arc Resistance 130 sec
130 sec
ASTM D495
Kolon KOPA® KN133G43SIBL G/F Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Arc Resistance 130 sec
130 sec
ASTM D495
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose
Feature: Injection Molding,PA6+GF30%, General PurposeApplication: Automotive (Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
Arc Resistance 130 sec
130 sec
ASTM D495
Kolon KOPA® KN333G15HI Multi Reinforced Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Arc Resistance 130 sec
130 sec
ASTM D495
Kolon SPESIN® KP213G15HIBL Impact Resistant PBT Compound resin
G/F 15% + Impact resistantApplications: SwitchesInformation provided by API-Kolon.
Arc Resistance 130 sec
130 sec
ASTM D495
LG Chemical Lupox® PBT-GP-1000 High Flow PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Arc Resistance 130 sec
130 sec
ASTM D495
Haysite HCR-191 Corrosion Resistant Polyester/Glass Sheet
A fiber glass reinforced thermoset sheet using HETRON 197® flame resistant polyester in the resin matrix. Standard color is light beige. Additional data covering resistance to specific chemicals ..
Arc Resistance 130 sec
130 sec
ASTM D495
Sumitomo Bakelite North America 73-70-70 C-P /73-70-70 VO-P Short-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I..
Arc Resistance 130 sec
130 sec
Absolute Drying; ASTM-D495
Toyobo GLAMIDE® TY-145TZ Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Arc Resistance 130 sec
130 sec
Absolute Drying; ASTM-D495
Toyobo GLAMIDE® TY-835TC Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Arc Resistance 130 sec
130 sec
Tungsten electrode; ASTM D495
Toyobo VYLOPET® EMC310TU Injection Molding Polyester Resin, Warpageless, High cycles
Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesWarpagelessInformation provided by Toyobo.
Arc Resistance 130 sec
130 sec
Tungsten electrode; ASTM D495
Toyobo VYLOPET® EMC341 Injection Molding Polyester Resin, Hydrolysis Resistant
Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo.
Arc Resistance 130 sec
130 sec
Tungsten electrode; ASTM D495
Toyobo VYLOPET® EMC407 Non-Reinforced
Applications: Iron's heat insulation plateChair framesHousingsFeatures: WarpagelessImproved processabilityHigh fluidityGood appearanceInformation provided by Toyobo.
Arc Resistance 130 sec
130 sec
ASTM D495
Unitika U-100 Engineering Plastic
CAS No: 26590-50-1Information provided by Unitika Ltd.
Arc Resistance 130 sec
130 sec
Dow Corning 4 ELECTRICAL INSULATING COMPOUND
Silicone-based compound, moderate consistency. Lubricant suitable for electrical connectors and joints.Information provided by Dow Corning
Arc Resistance 130 sec
130 sec
ASTM D495
Celanese CELANEX 1642Z PBT, 20% Glass Reinforced
Celanex 1642Z is a general purpose, 20% fiberglass reinforced PBT with a good balance of mechanical properties and processability.Information provided by Celanese
Arc Resistance 130 sec
130 sec
Internal
Celanese VECTRA A435 LCP, 35% Specialty
Best High Current Arc Ignition (HAI) performance. Glass/PTFE filled.Information provided by Celanese
Arc Resistance 130 sec
130 sec
ASTM D495
Chang Chun Plastic PBT3030 30% Glass Fiber Enforced PBT
Information provided by Dowell Trading Company Ltd.
Arc Resistance 130 sec
130 sec
Internal
Celanese VECTRA A430 LCP, 25% Specialty
Provides many of the characteristics of A130 with added lubricity. Suitable for applications requiring excellent wear characteristics. Excellent electrical properties at high frequencies. LCP/PTF..
Arc Resistance >= 130 sec
>= 130 sec
Bulk Molding Compounds BMC 2201 Mineral Filled Alkyd
BMC 2201 molding compound is a mineral filled, glass-fiber-and nylon-floc reinforced alkyd compound suitable for compression and transfer molding. It was developed for applications requiring better ..
Arc Resistance 130 sec
130 sec
ASTM D495
RTP Company RTP 207B  Nylon 6/10 (PA 6/10) Glass Fiber 40%  (discontinued **)
Glass Fiber 40%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Arc Resistance 130 sec
130 sec
ASTM D495
RTP Company RTP 209B  Nylon 6/10 (PA 6/10) Glass Fiber 50%  (discontinued **)
Glass Fiber 50%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Arc Resistance 130 sec
130 sec
ASTM D495
Plenco 7307 Phenolic, Granular, Transfer Molded
PLENCO 07307 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength properties. Type ASTM 5948 CFG, and UL recognized under component file E40654. 07307 is a..
Arc Resistance 130 sec
130 sec
ASTM D495
Kolon KOPA® KN3321G15VO G/F Reinforced & Flame Retardant Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstanding ..
Arc Resistance 130 sec
130 sec
ASTM D495
Celanese Celanex® 1642Z PBT, 20% Glass Reinforced
Celanex 1642Z is a general purpose, 20% fiberglass reinforced PBT with a good balance of mechanical properties and processability.Information provided by Celanese Corporation.