Electrical Properties | Metric | English | Comments |
---|---|---|---|
Static Decay | 2.00 sec | 2.00 sec | Average value: 2.00 sec Grade Count:5 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Static Decay | 2.00 sec | 2.00 sec | Average value: 2.00 sec Grade Count:5 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Static Decay | 2.00 sec | 2.00 sec | Average value: 2.00 sec Grade Count:13 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini.. |
|||
Static Decay | 2.00 sec | 2.00 sec | Average value: 2.00 sec Grade Count:4 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Static Decay | 2.00 sec | 2.00 sec | Average value: 2.00 sec Grade Count:3 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Static Decay | 2.00 sec | 2.00 sec | Average value: 2.00 sec Grade Count:6 |
Overview of materials for Polypropylene, Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu.. |
|||
Static Decay | 2.00 sec | 2.00 sec | Average value: 2.00 sec Grade Count:6 |
Overview of materials for Nylon 6, Stainless Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Stainless Steel Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Static Decay | 2.00 sec | 2.00 sec | Average value: 2.00 sec Grade Count:7 |
Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, NCG Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Static Decay | 2.00 sec | 2.00 sec | Average value: 2.00 sec Grade Count:6 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Static Decay | 2.00 sec | 2.00 sec | Average value: 2.00 sec Grade Count:13 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |
|||
Static Decay | 2.00 sec | 2.00 sec | Average value: 2.00 sec Grade Count:4 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Static Decay | 2.00 sec | 2.00 sec | Average value: 2.00 sec Grade Count:3 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |