Electrical Properties Metric English Comments
Shielding Effectiveness >= 40 dB

@Frequency 2.20e+7 - 3.00e+7 Hz
>= 40 dB

@Frequency 2.20e+7 - 3.00e+7 Hz
Parker Chomerics CHO-BUTTON® EMI Grounding Contact
Description: CHO-BUTTON® grounding contacts provide a reliable RF bond between metallic parts of an enclosure (side panels-to-frame, door-to-frame, etc). When spaced at 4 to 8 inch intervals, the s..
Shielding Effectiveness >= 40 dB

@Thickness 3.00 mm
>= 40 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics Lexan® NX07331 PC+ABS (Asia Pacific)
FARADEX NX07331 is a commercial grade EMI shielding material
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX AS002 ABS
LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding...
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Asia Pacific)
LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East)
LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX DS0036I PC
LNP* FARADEX* DS0036I is a compound based on Polycarbonate resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, No..
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX DS0036I PC (Europe-Africa-Middle East)
LNP* Faradex* DS0036I is a compound based on Polycarbonate resin containing Flame Retardant, Stainless Steel Fiber. Added features of this material include: High Impact, Flame Retardant, Non-Bromin..
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP Faradex DS0036IC PC (Europe-Africa-Middle East)
LNP* FARADEX* DS0036IC is a compound based on Polycarbonate resin, containing Stainless Steel Fiber, Flame Retardant. Added features include: Non-Brominated & Non-Chlorinated Flame Retardant, High I..
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP Faradex DS0036IP PC
LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B..
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP Faradex DS0036IP PC (Asia Pacific)
LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B..
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP Faradex DS0036IP PC (Europe-Africa-Middle East)
LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B..
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX DS0036IR PC (Europe-Africa-Middle East)
LNP* FARADEX* DS0036IR is a compound based on Polycarbonate resin containing Stainless Steel Fiber, Flame Retardant. Added features include: Improved Paintability, Non-Brominated & Non-Chlorinated F..
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX MS002 PP
LNP* FARADEX* MS002 is a compound based on Polypropylene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX MS002 PP (Asia Pacific)
LNP* Faradex* MS002 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP Faradex MS002P PP (Asia Pacific)
LNP* Faradex* MS002P is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Exceptional Processi..
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP Faradex MS002P PP (Europe-Africa-Middle East)
LNP* Faradex* MS002P is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Exceptional Processi..
Shielding Effectiveness >= 40 dB

@Thickness 3.00 mm
>= 40 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX NX07331 PC+ABS (Asia Pacific)
FARADEX NX07331 is a commercial grade EMI shielding material
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX MS002 PP (Europe-Africa-Middle East)
LNP* Faradex* MS002 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Shielding Effectiveness 40 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
40 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
ASTM D149
Techmer ES Electrablend® ABS 03007 Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: ESD ProtectionInformation provided by TP Composites, Inc.
Shielding Effectiveness 40 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
40 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
ASTM D149
Techmer ES Electrablend® ABS 03008 Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: ESD ProtectionInformation provided by TP Composites, Inc.
Shielding Effectiveness 40 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
40 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
ASTM D149
Techmer ES Electrablend® ABS 03010 Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: ESD Protection and Good MoldabilityInformation provided by TP Composites, Inc.
Shielding Effectiveness 40 dB
40 dB
ASTM D4935
Techmer ES Electrablend® ABS 04001 BK 10% Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 7965121I..
Shielding Effectiveness 40 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
40 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
ASTM D149
Techmer ES Electrablend® HDPE 04001 LE BK
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ESD Protection and ConductiveAppearance: BlackProcessing Method: ExtrusionInformation provided by ..
Shielding Effectiveness 40 dB
40 dB
ASTM D4935
Techmer ES Electrablend® PA6/6 GF13 SS10 BK 13/10% Glass/Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Stainless Steel Reinforcement, 13/10% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation..
Shielding Effectiveness 40 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
40 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
ASTM D149
Techmer ES Electrablend® PC SS10 10% Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: ConductiveInformation provided by TP Composites, Inc.
Shielding Effectiveness 40 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
40 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
ASTM D149
Techmer ES Electrablend® POM CO Acetal
Availability: North AmericaForms: PelletsFeatures: Copolymer and Medium ViscosityInformation provided by TP Composites, Inc.
Shielding Effectiveness 40 dB
40 dB
ASTM D4935
Techmer ES Electrablend® ABS SS10 FR BK 10% Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 10% Filler by WeightFeatures: Flame Retardant and Electromagnetic Shielding (EMI)Appearance: BlackInformation pr..
Shielding Effectiveness 40 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
40 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
ASTM D149
Techmer ES Electrablend® ABS SS7 BK MB 7% Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 7% Filler by WeightFeatures: ESD ProtectionAppearance: BlackInformation provided by TP Composites, Inc.
Shielding Effectiveness 40 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
40 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
ASTM D149
Techmer ES Electrablend® ABS SS7 MB 7% Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 7% Filler by WeightFeatures: ESD ProtectionInformation provided by TP Composites, Inc.
Copyright © lookpolymers.com All Rights Reserved