Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP FARADEX MS002 PP (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP FARADEX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP FARADEX MS002 PP (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Faradex* MS002 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
ISO 1183
1.12 g/cc
0.0405 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 15.0 MPa
2180 psi
ISO 527
Tensile Strength, Yield 19.0 MPa
2760 psi
ISO 527
Elongation at Break 70 %
70 %
ISO 527
Elongation at Yield 6.1 %
6.1 %
ISO 527
Tensile Modulus 1.20 GPa
174 ksi
1 mm/min; ISO 527
Flexural Strength 31.0 MPa
4500 psi
ISO 178
Flexural Modulus 1.40 GPa
203 ksi
ISO 178
Izod Impact, Notched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 100 kJ/m²
47.6 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 116 µm/m-°C

@Temperature -40.0 - 40.0 °C
64.4 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 156 µm/m-°C

@Temperature -40.0 - 40.0 °C
86.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C
133 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method