Polymer Property : Shielding Effectiveness = 55 dB Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Shielding Effectiveness 46 - 55 dB

@Frequency 1.00e+8 Hz
46 - 55 dB

@Frequency 1.00e+8 Hz
Parker Chomerics WIN-SHIELD™ ITO (Coated) EMI Shielded Window
Description: Parker Chomerics display windows and filters are available in various plastic materials, including polycarbonate, acrylic and cast allycarbonate. A unique feature of Parker Chomerics w..
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX AS002 ABS
LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding...
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Asia Pacific)
LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East)
LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX DS0036I PC
LNP* FARADEX* DS0036I is a compound based on Polycarbonate resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, No..
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX DS0036I PC (Europe-Africa-Middle East)
LNP* Faradex* DS0036I is a compound based on Polycarbonate resin containing Flame Retardant, Stainless Steel Fiber. Added features of this material include: High Impact, Flame Retardant, Non-Bromin..
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP Faradex DS0036IC PC (Europe-Africa-Middle East)
LNP* FARADEX* DS0036IC is a compound based on Polycarbonate resin, containing Stainless Steel Fiber, Flame Retardant. Added features include: Non-Brominated & Non-Chlorinated Flame Retardant, High I..
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP Faradex DS0036IP PC
LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B..
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP Faradex DS0036IP PC (Asia Pacific)
LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B..
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP Faradex DS0036IP PC (Europe-Africa-Middle East)
LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B..
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX DS0036IR PC (Europe-Africa-Middle East)
LNP* FARADEX* DS0036IR is a compound based on Polycarbonate resin containing Stainless Steel Fiber, Flame Retardant. Added features include: Improved Paintability, Non-Brominated & Non-Chlorinated F..
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX MS002 PP
LNP* FARADEX* MS002 is a compound based on Polypropylene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX MS002 PP (Asia Pacific)
LNP* Faradex* MS002 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP Faradex MS002P PP (Asia Pacific)
LNP* Faradex* MS002P is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Exceptional Processi..
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP Faradex MS002P PP (Europe-Africa-Middle East)
LNP* Faradex* MS002P is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Exceptional Processi..
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
SABIC Innovative Plastics LNP FARADEX MS002 PP (Europe-Africa-Middle East)
LNP* Faradex* MS002 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding.