Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 7.00 - 60.0 sec | 7.00 - 60.0 sec | Average value: 20.7 sec Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Hot Wire Ignition, HWI | 7.00 - 60.0 sec | 7.00 - 60.0 sec | Average value: 20.9 sec Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Hot Wire Ignition, HWI | 15.0 - 60.0 sec | 15.0 - 60.0 sec | Average value: 33.8 sec Grade Count:8 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Hot Wire Ignition, HWI | 15.0 - 60.0 sec | 15.0 - 60.0 sec | Average value: 41.1 sec Grade Count:25 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Hot Wire Ignition, HWI | 30.0 - 60.0 sec | 30.0 - 60.0 sec | Average value: 45.0 sec Grade Count:3 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
Hot Wire Ignition, HWI | 3.00 - 60.0 sec | 3.00 - 60.0 sec | Average value: 18.6 sec Grade Count:6 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Hot Wire Ignition, HWI | 7.00 - 60.0 sec | 7.00 - 60.0 sec | Average value: 20.9 sec Grade Count:3 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
Hot Wire Ignition, HWI | 7.00 - 60.0 sec | 7.00 - 60.0 sec | Average value: 26.8 sec Grade Count:4 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |