Arlon Thermabond® R36200A008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name Thermabond®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon Thermabond® R36200A008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated Fiberglass Appearance: Blue silicone gumThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 25.4 microns
1.00 mil
Liner
76.2 microns
3.00 mil
Carrier
203 microns
8.00 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Silicone Property; ASTM D2240
Tensile Strength 5.17 MPa
750 psi
Silicone Property; ASTM D412
Elongation at Break 450 %
450 %
Silicone Property; ASTM D412
Poissons Ratio 0.50
0.50
Approximately, Silicone Property
Shear Strength 5.86 MPa
850 psi
Lap Shear Strength; ASTM D1002
Thermal Properties Metric English Comments
CTE, linear 280 µm/m-°C
156 µin/in-°F
Silicone Property; ASTM E 831
Specific Heat Capacity 0.990 J/g-°C
0.237 BTU/lb-°F
E 1461-01
Thermal Conductivity 0.330 W/m-K
2.29 BTU-in/hr-ft²-°F
Silicone Property; ASTM E 1530
0.330 W/m-K
2.29 BTU-in/hr-ft²-°F
Product Property; ASTM E 1530
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -73.3 °C
-100 °F
Glass Transition Temp, Tg <= -100 °C
<= -148 °F
Silicone Property; ASTM D3418
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 3.3

@Frequency 1.00e+6 Hz
3.3

@Frequency 1.00e+6 Hz
D<sub>k</sub>, Silicone Property; IPC TM 650-2.5.5.3
Dielectric Strength 43.3 kV/mm
1100 kV/in
ASTM D149
Dissipation Factor 0.0046

@Frequency 1.00e+6 Hz
0.0046

@Frequency 1.00e+6 Hz
D<sub>f</sub>, Silicone Property; IPC TM 650-2.5.5.3
Processing Properties Metric English Comments
Cure Time 15.0 min

@Pressure >=0.689 MPa,
Temperature 121 °C
0.250 hour

@Pressure >=100 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 3.00 Month

@Temperature 4.44 - 10.0 °C
3.00 Month

@Temperature 40.0 - 50.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Blue
Total Product Weight (g/m2) 250
Arlon SQA-TMS-025