Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 13.8 kV/mm | 350 kV/in | |
Resinlab® CYNERGY CA6403 Adhesive Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | |
Resinlab® CYNERGY CA6405 Adhesive Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Dielectric Strength | 13.8 - 105 kV/mm | 350 - 2670 kV/in | Average value: 28.7 kV/mm Grade Count:20 |
Overview of materials for ECTFE Fluoropolymer This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Dielectric Strength | 13.8 - 19.7 kV/mm | 350 - 500 kV/in | Average value: 15.3 kV/mm Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Mar-Bal MB2000-15 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Mar-Bal MB4000 Thermoset Polyester Composite Molding Compound The high track resistant material. A flame retardant polyester molding compound with moderate strength and excellent electrical properties and exceptional arc and track resistance. Suitable for repl.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Mar-Bal MB5500 Thermoset Polyester Composite Molding Compound A superior heat resistant material. U.L. RTI rating of 160°C-170°C.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
ITW Devcon Flexane® Rubber Repair / Castable Urethane 80 Liquid, Black Information provided by ITW Devcon |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
ITW Devcon Flexane® Rubber Repair / Castable Urethane 80 Putty, Black Information provided by ITW Devcon |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
ITW Devcon Flexane® Rubber Repair / Castable Urethane Fast Cure, Black Information provided by ITW Devcon |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
ITW Devcon Rubber Repair / Castable Urethane Edge & Seal (T-35), Black Information provided by ITW Devcon |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | Short Term |
Saint-Gobain Rulon® II Bearing/Seal PTFE An injection moldable bearing material that possesses excellent chemical and wear resistance. Rulon II is available in injection molded finished parts only. Excellent friction and wear properties al.. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | Short Time; ASTM D149 |
Sumitomo Bakelite Durez® 153 Phenolic, Injection Grade Durez 153 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits good molded appearance and shock resistance for use on a wide variety of electrical a.. |
|||
Dielectric Strength | 13.8 kV/mm @Frequency 60.0 Hz |
351 kV/in @Frequency 60.0 Hz |
Wet, step by step; ASTM D149 |
Sumitomo Bakelite North America 73-70-70 C-P /73-70-70 VO-P Short-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | |
Cytec (Conap) FR-1050 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | |
Cytec (Conap) RN-1000 / EA-87 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Arlon 32140R062 0.062" (1.57 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer release linerThis data represents typical values for the production ma.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Arlon 56586R026 0.027" (0.686 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Red silicone gum and rubber on fiberglass clo.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Arlon 56606R026 0.027" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production materia.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | |
Arlon R30370A008 0.008" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.001" FEP FilmSide 1: Unsupported/Uncured Silicone RubberSubstrate: 0.003" PTFE coated FiberglassThis data represents typical values for the production material a.. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | ASTM D149 |
Chang Chun Plastic Longlite PM T376J Heat Resistant Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | S/T |
Abatron AboCast 8103-30 High-Performance Dielectric Epoxy AboCast 8103-30 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has high h.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | |
Arlon R30370A015 0.015" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.001" FEP FilmSide 1: Unsupported/Uncured Silicone RubberSubstrate: 0.003" PTFE coated FiberglassThis data represents typical values for the production material a.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | |
Trelleborg Emerson & Cuming Stycast® 2741-15 Two-Component Epoxy Flexible Encapsulant Emerson & Cuming 2741-15 Stycast® Two-Component Epoxy Flexible EncapsulantDescriptionElectronic embedment and sealing of metals, ceramics, and plastics. Protection of stress sensitive components wh.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Westlake Plastics Halar® 901 ECTFE Made from HALAR® ethylene-chlorotrifluoroethylene resin, these products are virtually unaffected by most corrosive chemicals. ECTFE products have excellent chemical and mechanical properties, impa.. |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | ASTM D149 |
Quantum Nylon 6/6 30% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |
|||
Dielectric Strength | 13.8 kV/mm | 350 kV/in | |
Resinlab® UR1049 MDI Based Rigid Polyurethane Foam System Resinlab™ UR 1049 is a, two component, water blown, 4 lb per cubic foot, MDI based rigid polyurethane foam system. It is designed to cure completely at room temperature. Being of a closed cell stru.. |
|||
Dielectric Strength | 13.8 kV/mm | 351 kV/in | 60 Hz, wet, SS; ASTM D149 |