Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 17.7 - 19.7 kV/mm | 450 - 500 kV/in | Average value: 18.2 kV/mm Grade Count:4 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |
|||
Dielectric Strength | 13.8 - 19.7 kV/mm | 350 - 500 kV/in | Average value: 15.3 kV/mm Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Dielectric Strength | 18.1 - 19.7 kV/mm | 460 - 500 kV/in | Average value: 19.5 kV/mm Grade Count:18 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Dielectric Strength | 17.7 - 19.7 kV/mm | 450 - 500 kV/in | |
Lord Adhesives Circalokâ„¢ 6031 A/B Epoxy Encapsulant Circalokâ„¢ 6031 A/B is a two-part epoxy potting compound with excellent electrical properties at elevated temperatures. Good arc-track resistance under high voltage loading and other dielectric .. |
|||
Dielectric Strength | 15.7 - 19.7 kV/mm @Thickness 3.17 mm |
400 - 500 kV/in @Thickness 0.125 in |
Short time value |
Abatron AboCast/AboCure 8109-3 Low viscosity, RT cure. Easy processing.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140.. |
|||
Dielectric Strength | 15.7 - 19.7 kV/mm @Thickness 3.17 mm |
400 - 500 kV/in @Thickness 0.125 in |
Short time value |
Abatron AboCast/AboCure 8109-8 All-purpose, structural dielectric resin. High thermal and chemical resistance and RT cure.Processing: 100/12 ratio; Potlife: 45 min/20°C (68°F), 20 min/40°C (105°F), 10 min /60°C (140°F); mi.. |
|||
Dielectric Strength | 15.7 - 19.7 kV/mm | 400 - 500 kV/in | |
Abatron AboCast 7802-1/AboCure 50-3 (40 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, .. |
|||
Dielectric Strength | 15.7 - 19.7 kV/mm | 400 - 500 kV/in | Average value: 17.7 kV/mm Grade Count:12 |
Overview of materials for Nylon 6, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Dielectric Strength | 14.2 - 19.7 kV/mm | 360 - 500 kV/in | Average value: 17.0 kV/mm Grade Count:7 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |