Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 7.87 kV/mm | 200 kV/in | |
CE Phenolic Laminate Cotton based phenolic provides more mechanical strength than paper grades and has a finer surface with better machinability. This material is used for gears, pinions, bearings, bushings, and many s.. |
|||
Dielectric Strength | >= 7.87 kV/mm | >= 200 kV/in | ASTM D149 |
Saint-Gobain Fluoroloy® A12 High Performance Seal Material Excellent wear and heat resistance; Non-abrasive; Recommended for moderate to high speed service running against soft or hard metals; Performs well against lubricated and non-lubricated surfacesInfo.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | ASTM D257 |
Ensinger Tecapeek® MT Polyetheretherketone (PEEK) TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | ASTM D149 |
Devcon Carbide Putty Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | ASTM D149 |
Arlon 25662T010 0.010" (0.254 mm) Cured Silicone Rubber with Laminated ETFE Film Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Laminated ETFE FilmChemical Compatibility: (ETFE offers good chemical resistance to the following classes of chemicals) Alkalis, Organic a.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | ASTM D1000 |
3M Bumpon™ SJ5816 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | ASTM D1000 |
3M Bumpon™ SJ5832 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | ASTM D1000 |
3M Bumpon™ SJ6008 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | ASTM D1000 |
3M Bumpon™ SJ6016 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | ASTM D1000 |
3M Bumpon™ SJ6032 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | ASTM D1000 |
3M Bumpon™ SJ6216 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | Perpendicular to Laminate Face; ASTM D149 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 1/8" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | Perpendicular to Laminate Face; ASTM D149 |
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 3/8" to 1" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | Perpendicular to Laminate Face; ASTM D149 |
Bedford Plastics Glass Reinforced Polyester Structural Fiberglass Profiles Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | Perpendicular to Laminate Face; ASTM D149 |
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 3/16" to 1/4" Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod.. |
|||
Dielectric Strength | 7.87 - 11.8 kV/mm | 200 - 300 kV/in | |
3M 4004 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Dielectric Strength | 7.87 - 11.8 kV/mm | 200 - 300 kV/in | |
3M 4008 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Dielectric Strength | 7.87 - 11.8 kV/mm | 200 - 300 kV/in | |
3M 4026 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Dielectric Strength | 7.87 - 11.8 kV/mm | 200 - 300 kV/in | |
3M 4052 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Dielectric Strength | 7.87 - 11.8 kV/mm | 200 - 300 kV/in | |
3M 4085 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | ASTM D1000 |
3M Bumpon™ SJ6208 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | Perpendicular to Laminate Face; ASTM D149 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet 1/8" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | Perpendicular to Laminate Face; ASTM D149 |
Bedford Plastics Glass Reinforced Polyester Flat Sheet, 3/8" to 1" Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | ASTM D1000 |
3M Bumpon™ SJ5808 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | Solvent Resistance |
3M MDT Tubing 3M MDT Tubing offers increased flexibility in combination with excellent abrasion, corrosion and environmental resistance properties and meets MIL-DTL-23053/15, Class 2. Uncoated product (without se.. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | Short Term |
Saint-Gobain Rulon® FCJ Grade Bearing/Seal PTFE
(discontinued **) Saint Gobain Rulon® CJ is now produced as a part of the TriStar Plastics Corp. product line under the CJ Bearings trade name.Description: Rulon® is the Saint-Gobain trade name for their family of .. |
|||
Dielectric Strength | 7.87 kV/mm | 200 kV/in | ASTM D149 |
Saint-Gobain Meldin® 2021 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |