Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 14.2 kV/mm @Thickness 3.17 mm |
361 kV/in @Thickness 0.125 in |
ASTM D149 |
ExxonMobil Escorene® LD-402 LDPE Electrical Jacketing Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low density polyethylene homopolymer resin designed for high speed extrusions. |
|||
Dielectric Strength | 14.2 kV/mm | 361 kV/in | ASTM D149 |
Plenco 201 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok 201 is a two-stage, woodflour and mineral-filled phenolic molding compound formulated to have an excellent balance of molded properties. The material provides good electrical insulation val.. |
|||
Dielectric Strength | 14.2 kV/mm | 361 kV/in | ASTM D149 |
Plaslok 201 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 201 is a two-stage, woodflour and min.. |
|||
Dielectric Strength | 14.2 kV/mm | 361 kV/in | ASTM D149 |
IDI Composites A-207 Thermoset Polyester, Sheet AUTOMOTIVE - Versatile family of compounds specifically designed for automotive structural applications. Low shrink characteristics, heat resistance, long-term dimensional stability, and corrosion r.. |
|||
Dielectric Strength | 14.2 kV/mm | 361 kV/in | ASTM D149 |
IDI Composites E-205 Thermoset Polyester, Sheet ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista.. |
|||
Dielectric Strength | 14.2 kV/mm | 361 kV/in | 60Hz, Step-by-Step, wet; ASTM D149 |
Sumitomo Bakelite North America E 8353-706R-1 Hardware Grade Epoxy Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Dielectric Strength | 14.2 kV/mm @Frequency 60.0 Hz |
361 kV/in @Frequency 60.0 Hz |
short time, dry; ASTM D149 |
Sumitomo Bakelite North America E 2748A Short Glass Fiber Reinforced Epoxy E 2748A is a glass reinforced epoxy molding compound, with good impact strength combined with soft flow for the encapsulation of devices requiring high quality and thermal shock resistance.Informati.. |
|||
Dielectric Strength | 14.2 kV/mm | 361 kV/in | Short Time; ASTM D149 |
Plenco 2308 Phenolic, Granular, Compression Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |
|||
Dielectric Strength | 14.2 kV/mm | 361 kV/in | Short Time; ASTM D149 |
Plenco 2408 Phenolic, Granular, Compression Molded PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component fi.. |
|||
Dielectric Strength | 14.2 - 16.2 kV/mm | 361 - 411 kV/in | short time |
Bulk Molding Compounds BMC T60-6002A-WG Wear Resistant Molding Compound BMC T60-6002A-WG is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost pe.. |
|||
Dielectric Strength | 14.2 - 16.2 kV/mm | 361 - 411 kV/in | short time |
Bulk Molding Compounds BMC T60-6002-WG(15) Wear Resistant Molding Compound BMC T60-6002-WG-(15) is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cos.. |
|||
Dielectric Strength | 14.2 kV/mm @Thickness 1.60 mm |
361 kV/in @Thickness 0.0630 in |
ASTM D149 |
E-Polymers SEPAZ® K115HF 15% Glass Fiber Reinforced High Flow PPS Resin Polyphenylene Sulfide Resin: High-performance engineering plastic SEPAZ PPS boasts excellent high-temperature resistance, flame retardancy and chemical resistance, physical strength, and its fluidit.. |