Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | >= 3.00 kV/mm | >= 76.2 kV/in | |
Paratherm Corporation Paratherm™ HE Heat Transfer Fluid Paratherm HE® is a high flash and fire point heat transfer fluid. Engineered for higher thermal and oxidative stability, it is efficient and cost effective. Its greater purity allows it to strong.. |
|||
Dielectric Strength | 3.00 - 4.00 kV/mm @Temperature 20.0 °C |
76.2 - 102 kV/in @Temperature 68.0 °F |
ASTM D877 |
Paratherm Corporation Paratherm™ NF Heat Transfer Fluid Description: Paratherm NF® heat transfer fluid is highly efficient, thermally stable and cost-effective. It is also non-fouling, low pour and odor free. Completely non-toxic, it is exceptionally .. |
|||
Dielectric Strength | 3.00 kV/mm @Thickness 2.00 mm |
76.2 kV/in @Thickness 0.0787 in |
IEC 243-1 |
LATI LATAN 13 K/30 30% Carbon Fiber Reinforced Polyoxymethylene Copolymer (POM)
(Unverified Data**) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Dielectric Strength | 3.00 - 37.0 kV/mm | 76.2 - 940 kV/in | Average value: 18.3 kV/mm Grade Count:24 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||
Dielectric Strength | 3.00 kV/mm | 76.2 kV/in | AC 60 Hz |
Fujipoly Industries Sarcon® 15GHR Thin-Film GHR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Dielectric Strength | 3.00 kV/mm | 76.2 kV/in | 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 15GHR Thin-Film GHR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Dielectric Strength | 3.00 kV/mm | 76.2 kV/in | 60°C for 500 hrs |
Fujipoly Industries Sarcon® 15GTR Thin-Film GTR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
Dielectric Strength | 3.00 kV/mm | 76.2 kV/in | AC 60 Hz; 200°C for 1,000 hrs |
Fujipoly Industries Sarcon® 15GTR Thin-Film GTR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |
|||
Dielectric Strength | 3.00 kV/mm | 76.2 kV/in | 1 in. axial in oil; ASTM D149 |
Glastic Laminates/Shapes HIR Grade HIR Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. Highest physical properties of GLASROD series. |
|||
Dielectric Strength | 3.00 kV/mm | 76.2 kV/in | 1 in. axial in oil; ASTM D149 |
Glastic Laminates/Shapes MTS Grade MTS Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. |
|||
Dielectric Strength | 3.00 kV/mm | 76.2 kV/in | 1 in. axial in oil; ASTM D149 |
Glastic Laminates/Shapes SG-200 Fiberglass-Reinforced Polyester Rod Data provided by Glastic Corporation.A continuous-filament fiberglass-roving provides superior strength. Excellent thermal endurance - used to replace silicone rod. |
|||
Dielectric Strength | 3.00 kV/mm | 76.2 kV/in | NF EN 60243.1 |
Isoflon Tisoflon® 3 AD Polytetrafluoroethylene Coated Glass Fabric PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon. |
|||
Dielectric Strength | 3.00 kV/mm | 76.2 kV/in | ASTM D149 |
Tipco Tipcolite® TMS 111 Phenolic Compound, Cellulose Pulp, in fluffy form, having Soft Flow & High Strength Soft Flow Phenolic Compound, Reinforced with Cellulose Pulp, in fluffy formApplications: Defence ApplicationsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industrie.. |
|||
Dielectric Strength | 3.00 kV/mm @Thickness 3.00 mm |
76.2 kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola Etronax DN Phenolic, Cotton Fabric Reinforcement, Brown, Tubes Description: A strong and tough material. Very low water absorption and the lowest swelling in water. Very good low-friction material. High wear resistance in aggressive and dust-filled environments.. |
|||
Dielectric Strength | 3.00 kV/mm @Thickness 3.00 mm |
76.2 kV/in @Thickness 0.118 in |
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1 |
Elektro-Isola Etronax MMF Phenolic, Cotton Fabric Reinforcement, Brown, Tubes Description: Mechanical applications. Reinforced with finer fabric than Etronax MF. Can be used, in particular, for mechanical applications where fine tolerances and smoother surface finish are requ.. |
|||
Dielectric Strength | 3.00 kV/mm | 76.2 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® HT2C-3X LF black 9833 PA6T/66-CF30 Product description: Grivory HT2C-3X LF black 9833 is a 30% carbon-fibre reinforced, PTFE modified engineering thermoplastic based on semicrystalline partially aromatic copolyamide. Polymer designat.. |
|||
Dielectric Strength | 3.00 kV/mm | 76.2 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® HT2C-3X LF black 9833 PA6T/66-CF30 Product description: Grivory HT2C-3X LF black 9833 is a 30% carbon-fibre reinforced, PTFE modified engineering thermoplastic based on semicrystalline partially aromatic copolyamide. Polymer designat.. |
|||
Dielectric Strength | 3.00 kV/mm | 76.2 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® XE 4102 black 9238 PA*-CF30 Grivory XE 4102 is a 30% carbon fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewab.. |
|||
Dielectric Strength | 3.00 kV/mm | 76.2 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® XE 4102 black 9238 PA*-CF30 Grivory XE 4102 is a 30% carbon fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewab.. |
|||
Dielectric Strength | 3.00 kV/mm | 76.2 kV/in | |
Accuratus Accuflect™ Light-Reflecting Ceramic Accuflect™ is a specially formulated and processed ceramic developed by Accuratus to satisfy the market demand for diffuse reflectors in high temperature and high energy environments.Key Property: .. |
|||
Dielectric Strength | 3.00 - 4.50 kV/mm @Temperature 90.0 °C |
76.2 - 114 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATG 115 Phenolic Molding Organic Filler, Compression Molded Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- Black, BrownSoft/medium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic .. |
|||
Dielectric Strength | 3.00 - 5.00 kV/mm @Temperature 90.0 °C |
76.2 - 127 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATM 125 Phenolic Molding Organic Filler, Compression Molded Characteristics:Glossy surface free of filler marks Surface good & free of flaws Good mouldabilitySurface free of filler marks even after turningGood mechanical strengthColor-black, brownSoft/medium.. |
|||
Dielectric Strength | 3.00 - 5.00 kV/mm @Temperature 90.0 °C |
76.2 - 127 kV/in @Temperature 194 °F |
IS 2584-1963 |
Amity Thermosets ATG 116 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- BlackMedium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic appliance ha.. |
|||
Dielectric Strength | 3.00 kV/mm | 76.2 kV/in | |
Von Roll Isola IMI Varnish 3405 Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.Flash Point: |
|||
Dielectric Strength | 3.00 - 23.0 kV/mm | 76.2 - 584 kV/in | Average value: 12.4 kV/mm Grade Count:4 |
Overview of materials for Polyimide, Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app.. |